| Ti-6Al-4V中界面能对α相片层生长的影响三维相场模拟 |
| 杨梅1,王刚2,滕春禹1,3,4, 徐东生1,张鉴5,杨锐1,王云志3 |
1. 中国科学院金属研究所, 沈阳 110016
2. 华南理工大学材料科学与工程学院, 广州 510640
3. The Ohio State University, Columbus OH 43210, USA
4. 东北大学理学院, 沈阳 110819
5. 中国科学院计算机网络信息中心, 北京 100190 |
|
| 3D PHASE FIELD SIMULATION OF EFFECT OF INTERFACIAL ENERGY ANISOTROPY ON SIDEPLATE GROWTH IN Ti–6Al–4V |
| YANG Mei 1, WANG Gang 2, TENG Chunyu 1,3,4, XU Dongsheng 1, ZHANG Jian 5, YANG Rui 1, WANG Yunzhi 3 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
2. School of Materials Science and Engineering, South China University of Technology, Guangzhou 510640
3. The Ohio State University, Columbus OH 43210, USA
4. College of Science, Northeastern University, Shenyang 110819
5. Computer Network Information Center, Chinese Academy of Sciences, Beijing 100190 |
引用本文:
杨梅 王刚 滕春禹 徐东生 张鉴 杨锐 王云志. Ti-6Al-4V中界面能对α相片层生长的影响三维相场模拟[J]. 金属学报, 2012, 48(2): 148-158.
,
,
,
,
,
.
3D PHASE FIELD SIMULATION OF EFFECT OF INTERFACIAL ENERGY ANISOTROPY ON SIDEPLATE GROWTH IN Ti–6Al–4V[J]. Acta Metall Sin, 2012, 48(2): 148-158.
| [1] Sastry S M L, Meschter P J, Oneal J E. Metall Mater Trans, 1984; 15A: 1451[2] Greenfie M A, Margolin H. Metall Trans, 1972; 3: 2649[3] Weiss I, Froes F H, Eylon D, Welsch G E. Metall Trans, 1986; 17A: 1935[4] Shell E, Semiatin S. Metall Mater Trans, 1999; 30A: 3219[5] Stefansson N, Semiatin S L, Eylon D. Metall Mater Trans, 2002; 33A: 3527[6] Stefansson N, Semiatin S L. Metall Mater Trans, 2003; 34A: 691[7] Yoder G R, Cooley L A, Crooker T W. Metall Mater Trans, 1977; 8A: 1737[8] Yoder G R, Cooley L A, Crooker T W. Eng Fract Mech, 1979; 11: 805[9] Lindigkeit J, Terlinde G, Gysler A, Lutjering G. Acta Metall, 1979; 27: 1717[10] Carter R D, Lee E W, Starke E A, Beevers C J. Metall Mater Trans, 1984; 15A: 555[11] Suresh S. Metall Mater Trans, 1985; 16A: 249[12] Hall I W, Hammond C. Mater Sci Eng, 1978; 32: 241[13] Ravichandran K S. Acta Metall Mater, 1991; 39: 401[14] Shademan S, Sinha V, Soboyejo A B O, Soboyejo W O. Mech Mater, 2004; 36: 161[15] Ma Y J. PhD Thesis, Institute of Metal Research, Chinese academy of sciences, Shenyang, 2009(马英杰. 中国科学院金属研究所博士学位论文, 沈阳, 2009)[16] Liu J R. Post–doctoral Research Report, Institute of Metal Research, Chinese academy of sciences, Shenyang, 2011(刘建荣.中国科学院金属研究所博士后出站报告, 沈阳, 2011)[17] Filip R, Kubiak K, ZiajaW, Sieniawski J. J Mater Process Technol, 2003; 133: 84[18] Li S K, Xiong B Q, Hui S X, Ye W J, Yu Y. Mater Sci Eng, 2007; A460: 140[19] Semiatin S L, Bieler T R. Acta Mater, 2001; 49: 3565[20] Ahmed T, Rack H J. Mater Sci Eng, 1998; A243: 206[21] Banerjee R, Bhattacharyya D, Collins P C, Viswanathan G B, Fraser H L. Acta Mater, 2004; 52: 377[22] Bhattacharyya D, Viswanathan G B, Fraser H L. Acta Mater, 2007; 55: 6765[23] Krahe P R, Aaronson H I, Kinsman K R. Acta Metall, 1972; 20: 1109[24] Zener C. Trans AIME, 1946; 167: 550[25] Kirkaldy J S. Scand J Metall, 1991; 20: 50[26] Aaronson H I, Furuhara T, Enomoto M. Scand J Metall, 1991; 20: 18[27] Mullins W W, Sekerka R F. J Appl Phys, 1963; 34: 323[28] Loginova I, Agren J, Amberg G. Acta Mater, 2004; 52: 4055[29] Ma N. PhD Thesis, The Ohio State University, 2005[30] Wang Y, Ma N, Chen Q, Zhang F, Chen S L, Chang Y A. JOM, 2005; 57: 32[31] Ma N, Yang F, Shen C,Wang G, Viswanathan G B, Collins P C, Xu D S, Yang R, Fraser H L,Wang Y Z. In: NinomiM ed., Ti–2007 Science and Technology, Sendai: the JapanInstitute of Metals, 2007: 287[32] Wang G, Xu D S, Yang R. Acta Phys Sin, 2009; 58(Spec): S343(王刚, 徐东生, 杨锐. 物理学报, 2009; 58: S343)[33] Chen Q, Ma N, Wu K S, Wang Y Z. Scr Mater, 2004; 50: 471[34] Mills M J, Hou D H, Suri S, Viswanathan G B. In: Pond R C ed., Boundaries and Interfaces in Materials: The David A. Smith Symposium, Warrendale: Minerals, Metals& Materials Soc, 1998: 295 |
|