| 低碳钢表面激光直接镀Ti层中裂纹形成的研究 |
| 许恒栋1,赵海燕1,S¨orn Ocylok2, Igor Kelbassa 2 |
1. 清华大学机械工程系, 北京100084
2.Fraunhofer Institute of Laser Technology, Aachen, Germany 52074 |
|
| STUDY ON CRACKS IN LASER DIRECT–CLADDED TITANIUM LAYER ON LOW CARBON STEEL |
| XU Hengdong 1, ZHAO Haiyan1,S¨orn Ocylok2, Igor Kelbassa2 |
1.Department of Mechanical Engineering, Tsinghua University, Beijing 100084
2.Fraunhofer Institute of Laser Technology, Aachen, Germany, 52074 |
引用本文:
许恒栋 赵海燕 S¨orn Ocylok Igor Kelbassa. 低碳钢表面激光直接镀Ti层中裂纹形成的研究[J]. 金属学报, 2012, 48(2): 142-147.
,
.
STUDY ON CRACKS IN LASER DIRECT–CLADDED TITANIUM LAYER ON LOW CARBON STEEL[J]. Acta Metall Sin, 2012, 48(2): 142-147.
| [1] Draugelates U, Bouaifi B, Wesling V. Mater Corros, 1992; 43: 166[2] Draugelates U, Bouaifi B, Steinberg H. Mater Corros, 1993; 44: 269[3] Steinberg H. PhD Thesis, Technology University of Clausthal, Clausthal, 1996[4] Chen Z K, Liu M, Zeng D C, Ma W Y. Laser J, 2009; 30: 55(陈志坤, 刘敏, 曾德长, 马文有. 激光杂志, 2009; 30: 55)[5] Chen H, Pan C X, Pan L, Tao X L. Heat Treat Met, 2002; 27: 5(陈浩, 潘春旭, 潘邻, 陶锡麒. 金属热处理, 2002; 27: 5)[6] Ghosh M, Chatterjee S. Mater Sci Eng, 2003; A358: 152[7] Kato H, Abe S, Tomizawa T. J Mater Sci, 1997; 32: 5225[8] Aleman B, Guitterrez I, Urcola J J. Mater Sci Technol, 1993; 36: 509[9] Ghosh M, Kundu S, Chatterjee S, Mishra B. Mater Trans, 2005; 36A: 1891[10] Kundu S, Chatterjee S. Mater Sci Eng, 2006; A425: 107[11] Changqing A, Zangpeng J. J Less Common Mater, 1990; 162: 315[12] Kundu S, Ghosh M, Laik A, Bhammurthy K, Kale G B, Chatterjee S. Mater Sci Eng, 2005; A407: 154[13] Kamat G R. Weld J, 1988; 67: 44[14] Tang R Z, Tian R Z. Binary Alloy Phase Diagram and Crystal Structure of Intermediate Phase. Changsha: Center South University Press, 2009: 551(唐仁政, 田荣璋 编. 二元合金相图及中间相晶体结构. 长沙: 中南大学出版社,2009: 551)[15] Li W, Zhang R L. J Changchun Univ, 1999; 9: 12(李文, 张瑞林, 长春大学学报, 1999; 9: 12)[16] Jiang S Y, Li S C. Rare Met Mater Eng, 2011; 40: 36(蒋淑英, 李世春, 稀有金属材料与工程, 2011; 40: 36)[17] Practical Handbook of Engineering Materials Editorial Board. Practical Handbook of Engineering Materials. 2nd Ed., Beijing: Standards Press of China, 2002: 8(工程材料实用手册编委会. 工程材料实用手册(第2版). 北京: 中国标准出版社, 2002: 8)[18] Shi C X, Li H D, Zhou L. Handbook of Materials Science and Engineering. Beijing: Chemical Industry Press, 2004: 1(师昌绪, 李恒德, 周廉. 材料科学与工程手册. 北京: 化学工业出版社, 2004: 1)[19] Zhu X K, Chao Y J. Comput Struct, 2002; 80: 967[20] Zhou Z F, Zhang W Y. Welding Metallurgy and Metal Welding Characteristics. 2nd Ed., Beijing: Mechanical Industry Press, 1988: 196(周振丰, 张文钺 合编, 焊接冶金与金属焊接性(第2版). 北京: 机械工业出版社, 1988: 196) |
|