| 定向凝固多孔铜热沉传热性能的理论分析 |
| 陈刘涛, 张华伟, 刘源, 李言祥 |
| 清华大学机械工程系, 先进成形制造教育部重点实验室, 北京 100084 |
|
| THEORETICAL STUDY ON HEAT TRANSFER PERFORMANCE OF DIRECTIOANLLY SOLIDIFIED POROUS COPPER HEAT SINK |
| CHEN Liutao, ZHANG Huawei, LIU Yuan, LI Yanxiang |
| Key Laboratory for Advanced Materials Processing Technology, Ministry of Education, Department of Mechanical Engineering, Tsinghua University, Beijing 100084 |
引用本文:
陈刘涛 张华伟 刘源 李言祥. 定向凝固多孔铜热沉传热性能的理论分析[J]. 金属学报, 2012, 48(11): 1374-1380.
CHEN Liutao ZHANG Huawei LIU Yuan LI Yanxiang.
THEORETICAL STUDY ON HEAT TRANSFER PERFORMANCE OF DIRECTIOANLLY SOLIDIFIED POROUS COPPER HEAT SINK[J]. Acta Metall Sin, 2012, 48(11): 1374-1380.
| [1] Mahajan R, Nair R, Wakharkar V, Swan J, Tang J, Vandentop G. Int Technol J Semicond Technol Manuf, 2002; 6: 61[2] Tuckerman D B, Pease R F W. IEEE Electron Dev Lett, 1981; 2: 126[3] Rosa P, Karayiannis T G, Collins M W. Appl Therm Eng, 2009; 29: 3447[4] Wei X J. J Electron Packag, 2004; 126: 60[5] Ogushi T, Chiba H, Nakajima H, Ikeda T. J Appl Phys, 2004; 95: 5843[6] Chiba H, Ogushi T, Nakajima H, Torji K, Tomimura T, Ono F. J Appl Phys, 2008; 103: 013515[7] Liu Y, Li Y X, Zhang H W, Wang J. Acta Metall Sin, 2005; 41: 886(刘源, 李言祥, 张华伟, 万疆. 金属学报, 2005; 41: 886)[8] Liu Y, Li Y X, Wan J, Zhang H W. Mater Sci Eng, 2005; A402: 47[9] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2006; 42: 1165(张华伟, 李言祥, 刘源. 金属学报, 2006; 42: 1165)[10] Li Y X, Liu Y, Zhang H W, Wang X. In: Nakajima H, Kanetake N eds., Proc Met Foam 2005, Sendai: The Japan Institute of Metals, 2006: 237[11] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2006; 42: 1171(张华伟, 李言祥, 刘 源. 金属学报, 2006; 42: 1171)[12] Wang X, Li Y X, Liu Y. Acta Metall Sin, 2006; 42: 1075(王雪, 李言祥, 刘源. 金属学报, 2006; 42: 1075)[13] Ogushi T, Chiba H, Nakajima H. In: Nakajima H, Kanetake N eds., Proc Met Foam 2005, Sendai: The Japan Institute of Metals, 2006: 27[14] Chiba H, Ogushi T, Nakajima H. In: Nakajima H, KanetakeN eds., Proc Met Foam 2005, Sendai: The Japan Institute of Metals, 2006: 35[15] Chen L T, Zhang H W, Liu Y, Li Y X. Acta Metall Sin, 2012: 48: 329(陈刘涛, 张华伟, 刘源, 李言祥. 金属学报, 2012: 48: 329)[16] Yang S M, Tao W Q. Heat Transfer. 4th Ed, Beijing: Higher Education Press, 2006: 57(杨世铭, 陶文铨. 传热学. 第4版, 北京: 高等教育出版社, 2006: 57)[17] Shah R K, London A L. Laminar Flow Forced Convection In Ducts. New York: Academic Press, 1978: 148[18] Li X Q, Li Y, Ding T. Engineering Fluid Mechanics. Beijing: China Water Power Press, 2009: 120(李小芹, 李 岩, 丁 涛. 工程流体力学. 北京: 中国水利水电出版社, 2009: 120) |
|