| 交变电场脉冲钝化Fe24Mn4Al5Cr反铁磁定膨胀合金及其耐蚀性研究 |
| 朱雪梅, 曹雪梅, 刘明, 雷明凯, 张彦生 |
1) 大连交通大学材料科学与工程学院, 大连 116028
2) 大连理工大学材料科学与工程学院表面工程实验室, 大连 116024 |
|
| AN ANTIFERROMAGNETIC Fe24Mn4Al5Cr COVAR ALLOY IMPULSE--PASSIVATED BY AN ALTERNATING CURRENT VOLTAGE OVERLAPPING A DIRECT CURRENT VOLTAGE AND ITS CORROSION RESISTANCE |
| ZHU Xuemei, CAO Xuemei, LIU Ming, LEI Mingkai, ZHANG Yansheng |
1) School of Materials Science and Engineering, Dalian Jiaotong University, Dalian 116028
2) Surface Engineering Laboratory, School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024 |
引用本文:
朱雪梅 曹雪梅 刘明 雷明凯 张彦生. 交变电场脉冲钝化Fe24Mn4Al5Cr反铁磁定膨胀合金及其耐蚀性研究[J]. 金属学报, 2012, 48(11): 1357-1364.
ZHU Xuemei CAO Xuemei LIU Ming LEI Mingkai ZHANG Yansheng.
AN ANTIFERROMAGNETIC Fe24Mn4Al5Cr COVAR ALLOY IMPULSE--PASSIVATED BY AN ALTERNATING CURRENT VOLTAGE OVERLAPPING A DIRECT CURRENT VOLTAGE AND ITS CORROSION RESISTANCE[J]. Acta Metall Sin, 2012, 48(11): 1357-1364.
| [1] Shi C X, Zhang Y S. Encycl Mater Sci Eng, 1993; 3(Suppl.): 1719[2] Casteletti L C, Lombardi N A, Totten G E, Heck S C, Fernandes F A P. J ASTM Int, 2010; 7: 102605[3] Zhu X M, Zhang Y S. Corrosion, 1998; 54: 3[4] Umino R, Liu X J, Sutou Y, Wang C P, Ohnuma I, Kainuma R, Ishida K. J Phase Equilb Diffus, 2006; 27: 54[5] Gebhardt T, Music D, Kossmann D, Ekholm M, Abrikosov I A, Vitos L, Schneider J M. Acta Mater, 2011; 59: 3145[6] Lee J W, Duh J G, Wang J H. Surf Coat Technol, 2003; 168: 223[7] Jaw J H, Cheng W C, Wang C J. Metall Mater Trans, 2005; 36A: 2289[8] Su C W, Lee J W, Wang C S, Chao C G, Liu T F. Surf Coat Technol, 2008; 202: 1847[9] Wang C H, Luo C W, Huang C F, Huang M S, Ou K L, Yu C H. J Alloys Compd, 2011; 509: 691[10] Zhang Y S, Zhu X M, Liu M, Che R X. Appl Surf Sci, 2004; 222: 89[11] Zhu X M, Liu M, Zhang Y S. Corros Eng Sci Technol, 2007; 42: 22[12] Wendt J L, Chin D T. Corros Sci, 1985; 25: 889[13] Wendt J L, Chin D T. Corros Sci, 1985; 25: 901[14] Song G L, Cao C N, Wang Y, Lin H C. J Chin Soc Corros Protect, 1991; 11: 319(宋光铃, 曹楚南, 王友, 林海潮. 中国腐蚀与防护学报, 1991; 11: 319)[15] Song G L, Cao C N, Lin H C, Xia B J. J Chin Soc Corros Protect, 1992; 12: 77(宋光铃, 曹楚南, 林海潮, 夏邦杰. 中国腐蚀与防护学报, 1992; 12: 77)[16] Mansfeld F, Lin S H, Kwiatkowski L. Corrosion, 1994; 50: 838[17] Zhang J X, Yan L C, Wei Z F, Qiao Y N, Cao C N, Zhang J Q. Acta Metall Sin, 2004; 40: 404(张俊喜, 颜立成, 魏增福, 乔亦男, 曹楚南, 张鉴清. 金属学报, 2004; 40: 404)[18] Taveira L V, Montemor M F, Belo M D C, Ferreira M G, Dick L F P. Corros Sci, 2010; 52: 2813[19] Doff J, Archibong P E, Jones G, Koroleva E V, Skeldon P, Thompson G E. Electrochim Acta, 2011; 56: 3225[20] Liu X L, Xu Y X, Zhang T, Shao Y W, Meng G Z, Wang F H. Corros Sci Prot Technol, 2009; 21: 188(刘晓兰, 徐雅欣, 张 涛, 邵亚薇, 孟国哲, 王福会. 腐蚀科学与防护技术, 2009; 21: 188)[21] Liu X L, Zhang T, Shao Y W, Meng G Z, Wang F H. Corros Sci, 2009; 51: 2685[22] Sanz J M, Hofmann S. Surf Interface Anal, 1986; 8: 147[23] Zhu X M, Zhang Y S. Appl Surf Sci, 1998; 125: 11[24] Trompette J L, Massot L. Corros Sci, 2012; 57: 174[25] Li Y C, Yan C W, Duan H P. J Chin Soc Corros Protect, 2002; 22: 375(李运超, 严川伟, 段红平. 中国腐蚀与防护学报, 2002; 22: 375)[26] Brug J, van den Eeden ALG, Sluyters–Rehbach M, Sluyters J H. J Electroanal Chem, 1984; 176: 275 |
|