镍基单晶高温合金杂晶形成倾向性的研究 |
张小丽,周亦胄,金涛,孙晓峰 |
中国科学院金属研究所, 沈阳 110016 |
|
STUDY ON THE TENDENCY OF STRAY GRAIN FORMATION OF Ni–BASED SINGLE CRYSTAL SUPERALLOYS |
ZHANG Xiaoli, ZHOU Yizhou, JIN Tao, SUN Xiaofeng |
Institute of Metal Research, Chinese Academy of Science, Shenyang 110016 |
引用本文:
张小丽 周亦胄 金涛 孙晓峰. 镍基单晶高温合金杂晶形成倾向性的研究[J]. 金属学报, 2012, 48(10): 1229-1236.
ZHANG Xiaoli ZHOU Yizhou JIN Tao SUN Xiaofeng.
STUDY ON THE TENDENCY OF STRAY GRAIN FORMATION OF Ni–BASED SINGLE CRYSTAL SUPERALLOYS[J]. Acta Metall Sin, 2012, 48(10): 1229-1236.
[1] Reed R C. The Superalloys Fundamentals and Applications. Cambridge: Cambridge University Press, 2006: 141
[2] Schafrik R E, Walston S. In: Reed R C, Green K A, Caron P, Gabb T P, Fahrmann M G, Huron E S, Woodard S A, eds., Superalloys 2008. Warrendale, PA: TMS, 2008: 3
[3] McLean M. Directionally Solidified Materials for High Temperature Service. London: The Metals Society, 1983: 161
[4] Shalin R E, Svetlov I L, Kachanov E B, Toloraiia V N, Gavrilin O S. Single Crystals of Nickel Superalloys. Moscow: Mocshinostroeniye, 1997: 336
[5] Fullagar K P L, Broomfield R W, Hulands M, Harris K, Erickson G L, Sikkenga S L. Trans ASME, 1996; 118: 380
[6] Goulette M J, Spilling P O, Arthey R P. In: Gill M, Kortovich C S, Briknell R H, Kent W B, Radavich J F, eds., Proc 5th International Symposium on Superalloys, Warrendale,
PA: TMS, 1984: 167
[7] de Bussac A, Gandin C A. Mater Sci Eng, 1997; A237: 35
[8] Goldschmidt D, Paul U, Sahm P R. In: Antolovich S D, Stusrud RW, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom eds., Superalloys 1992. Warrendale, PA:
TMS, 1992: 155
[9] Napolitano R E, Schaefer R J. Mater Sci, 2000; 35: 1641
[10] Bussac A D, Gandin C A. Mater Sci Eng, 1997; A237: 35
[11] Yang X L, Dong H B, Wang W, Lee P D. Mater Sci Eng, 2004; A386: 129
[12] Rappaz M, Gandin C A, Desbiolles J L, Thevoz P. Metall Mater Trans, 1996; 27A: 695
[13] Gandin C A, Schaefer R J, Rappaz M. Acta Mater, 1996; 44: 3333
[14] Pollock T M, Murphy W H, Goldman E H, Uram D L, Tu J S. In: Antolovich S D, Stusrud R W, MacKay R A, Anton D L, Khan T, Kissinger R D, Klarstrom D L eds.,
Superalloys 1992. Warrendale, PA: TMS, 1992: 125
[15] Pollock T M, Murphy W H. Metall Mater Trans, 1996; 27A: 1081
[16] Tin S, Pollock T M. Metall Mater Trans, 2003; 34A: 1953
[17] Gu J P, Beckermann C, Giamei A. Metall Mater Trans, 1997; 28A: 1533
[18] Copley S M, Giamei A F, Johnson S M, Hornbecker M F. Metall Trans, 1970; 1: 2193
[19] Zhou Y Z. Scr Mater, 2011; 65: 281
[20] D’Souza N, Jennings P A, Yang X L, Dong H B, Lee P D, McLean M. Metall Mater Trans, 2005; 36B: 657
[21] D’Souza N, Ardakani M G, McLean M, Shollock B A. Metall Mater Trans, 2000; 31A: 2877
[22] Napolitano R E, Schaefer R J. J Mater Sci, 2000; 35: 1641
[23] Meyer ter Vehn M, Dedecke D, Paul U, Sahm P R. In: Kissinger R D, Deye D J, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A, eds., Superalloys 1996.
Warrendale, PA: TMS, 1996: 471
[24] Cockcroft S L, Rappaz M, Mitchell A, Fernihough J, Schmalz A. In: Coutsouradis D, Davidson J H, Ewald J, Greenfield P, Khan T, Malik M, Meadowcroft D B, Regis
V, Scarlin R B, Schubert F, Thornton D V. Proc Materials for Advanced Power Engineering, Liege: Kluwer Academic publishers, 1994: 1145
[25] Kurz W, Fisher D J. Fundamentals of Solidification. Switzerland: Trans Tech Publications, 1984: 21
[26] Ma D X, Buhrig–Polaczek A. Metall Mater Trans, 2009; 40B: 738
[27] Paul U, Sahm P R. Mater Sci Eng, 1993; A173: 49
[28] Paul U, Sahm P R, Donner A, Goldschm D, Portella P D. Proc 2nd Symposium Materialforschung. Dresden: TUV Rheinland, k¨oln, 1991: 841 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|