| HRS和LMC工艺制备的两种镍基单晶高温合金铸态及固溶微孔的形成 |
| 石倩颖1,2,李相辉3,郑运荣2,谢光4, 张健4,5, 冯强1,2 |
1. 北京科技大学新金属材料国家重点实验室, 北京 100083\par
2. 北京科技大学国家材料服役安全科学中心, 北京 100083\par
3. 北京航空材料研究院先进高温结构材料重点实验室, 北京 100095\par
4. 中国科学院金属研究所高温合金部, 沈阳 110016\par
5. 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016 |
|
| FORMATION OF SOLIDIFICATION AND HOMOGENISATION MICROPORES IN TWO SINGLE CRYSTAL SUPERALLOYS PRODUCED BY HRS AND LMC PROCESSES |
| SHI Qianying 1,2, LI Xianghui 3, ZHENG Yunrong 2, XIE Guang 4,ZHANG Jian 4,5, FENG Qiang 1,2 |
1. State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083
2. National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083
3. Science and Technology on Advanced High Temperature Structural Material, Beijing Institute of Aeronautical Materials, Beijing 100095
4. Superalloys Division, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
5. Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
石倩颖 李相辉 郑运荣 谢光 张健 冯强. HRS和LMC工艺制备的两种镍基单晶高温合金铸态及固溶微孔的形成[J]. 金属学报, 2012, 48(10): 1237-1247.
| [1] Hu Z Q, Liu L R, Jin T, Sun X F. Aerial Eng, 2005; 31(3): 1(胡壮麒, 刘丽荣, 金涛, 孙晓峰. 航空发动机, 2005; 31(3): 1)[2] Pollock T M, Tin S. J Propul Power, 2006; 22: 361[3] Guo J T. Materials Science and Engineering for Superalloys (Vol.1). Beijing: Science Press, 2008: 387(郭建亭. 高温合金材料学(上册). 北京: 科学出版社, 2008: 387)[4] Chen Q Z, Jones N, Knowles D M. Acta Mater, 2002; 50: 1095[5] MacLachlan D W, Knowles D M. Mater Sci Eng, 2001; A302: 275[6] Wang Z H, Zhao N R, Li J G, Hou G C, Jin T, Sun X F, Hu Z Q. J Mater Eng, 2008; (12): 46(王志辉, 赵乃仁, 李金国, 侯贵臣, 金涛, 孙晓峰, 胡壮麒. 材料工程, 2008; (12): 46)[7] Ott M, Mughrabi H. Mater Sci Eng, 1999; A272: 24[8] Gayda J, Miner R V. Int J Fatigue, 1983; 5(3): 135[9] Anton D L. Acta Metall, 1984; 32: 1669[10] Link T, Zabler S, Epishin A, Haibel A, Bansal M, Thibault X. Mater Sci Eng, 2006; A425: 47[11] Lecomte–Beckers J. Metall Mater Trans, 1988; 19A: 2341[12] Anton D L, Giamei A F. Mater Sci Eng, 1985; 76: 173[13] Bokstein B S, Epishin A I, Link T, Esin V A, Rodin A O, Svetlov I L. Scr Mater, 2007; 57: 801[14] Toloraya V N, Svetlov I L. Metally, 1991; 5: 70[15] Komenda J, Henderson P J. Scr Mater, 1997; 37: 1821[16] Epishin A, Link T. Philos Mag, 2004; 84: 1979[17] Zhang J, Li J, Jin T, Sun X, Hu Z. J Mater Sci Technol, 2010; 26: 889[18] Wilson B C, Cutler E R, Fuchs G E. Mater Sci Eng, 2008;A479: 356[19] Liu L R, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Mater Lett, 2004; 58: 2290[20] Lamm M, Singer R F. Metall Mater Trans, 2007; 38A: 1177[21] Fritzemeier L G. In: Duhl D N, Maurer G, Antolovich S, Lund C, Reichman S, eds., Superalloys 1988, Chamption, PA: TMS, 1988: 265[22] Chen Q Z, Kong Y H, Jones C N, Knowles DM. Scr Mater, 2004; 51: 155[23] Elliott A J, Pollock T M. Metall Mater Trans, 2007; 38A: 871[24] Brundidge C L, Vandrasek D, Wang B, Pollock T M. Metall Mater Trans, 2012; 43A: 965[25] Elliott A, Pollock T, Tin S, King W, Huang S C, Gigliotti M. Metall Mater Trans, 2004; 35A: 3221[26] Lohm¨uller A, Eber W, Grobmann J, Hoerdler M, Preuhs J, Singer R. In: Green K A, Pollock T M, Kissinger R D, eds., Superalloys 2000, Champion, PA: TMS, 2000: 181[27] Grossman J, Preuhs J, Esser W, Singer R F. In: Mitchell A, Ridgway L, Baldwin M, eds., Symposium Liquid Metal Processing Casting, New York, NY: AVS, 1999: 31[28] Elliott A J, Feng G, Balsone S J, Schaeffer J C, Pollock T M, Gigliotti M F X. In: Srivatsan T S, ed., Processing and Fabrication of Advanced Materials XIV With Frontiers inMaterials Science 2005, Pittsburgh, PA: TMS, 2005, 267[29] Tang W S, Shen J, Wang D W, Zhang J, Lou L H. In: The Minerals, Metals & Materials Society, eds., TMS 2009 138th TMS Annual Meeting and Exhibition–SupplementalProceedings, Vol.1: Materials Proceeding and Properties, San Francisco, CA: TMS, 2009: 241[30] Liu C, Li K W, Shen J, Zhang J, Lou L H. Metall Mater Trans, 2012; 43A: 405[31] Kurz W, Fisher D J. Acta Metall, 1981; 29: 11[32] Feng Q, Carroll L J, Pollock T M. Metall Mater Trans, 2006; 37A: 1949[33] Hussain N, Shahid K A, Khan I H, Rahman S. Oxid Met, 1995; 43: 363[34] Weber J H, Gilman P S. Scr Metall, 1984; 18: 479[35] Rosenstein A, Tien J, Nix W. Metall Mater Trans, 1986; 17A: 151[36] Levy M, Farrell P, Pettit F. Corrosion, 1986; 42: 708[37] Karunaratne M S A, Cox D C, Carter P, Reed R C. In: Green K A, Pollock T M, Kissinger R D, eds., Superalloys 2000, Champion, PA: TMS, 2000: 263 |
|