| 强流脉冲离子束辐照WC-Ni硬质密封材料表面改性研究 |
| 张锋刚, 朱小鹏, 王明阳, 雷明凯 |
| 大连理工大学材料科学与工程学院表面工程研究室, 大连 116024 |
|
| SURFACE MODIFICATION OF WC-Ni CEMENTED CARBIDE FOR SEALS BY HIGH-INTENSITY PULSED ION BEAM IRRADIATION |
| ZHANG Fenggang, ZHU Xiaopeng, WANG Mingyang, LEI Mingkai |
| Surface Engineering Laboratory, School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024 |
引用本文:
张锋刚 朱小鹏 王明阳 雷明凯. 强流脉冲离子束辐照WC-Ni硬质密封材料表面改性研究[J]. 金属学报, 2011, 47(7): 958-964.
.
SURFACE MODIFICATION OF WC-Ni CEMENTED CARBIDE FOR SEALS BY HIGH-INTENSITY PULSED ION BEAM IRRADIATION[J]. Acta Metall Sin, 2011, 47(7): 958-964.
| [1] Cappelli E, Orlando S, Pinzari F, Napoli A, Kaciulis S. Appl Surf Sci, 1999; 138–139: 376[2] Karatas C, Yilbas B S, Aleem A, Ahsan M, Kaciulis S. J Mater Process Technol, 2007; 183: 234[3] Li T J, Lou Q H, Dong J X, Wei Y R, Liu J R. Appl Surf Sci, 2001; 172: 51[4] Gnyusov S, Tarasov S, Ivanov Yu, Rothstein V. Wear, 2004; 257: 97[5] Kano S, Inoue T. Surf Coat Technol, 2004; 257: 97[6] Gnyusov S, Tarasov S, Ivanov Yu, Rothstein V. Wear, 2004; 257: 97[7] Davis H A, Remnev G E, Stinnett R W, Yatsui K. MRS Bull, 1996; 21: 58[8] Yilbas B S, Shuja S Z, Arif A, Gondal M A. J Mater Process Technol, 2003; 135: 6[9] Lei M K, Zhu X P, Liu C, Xin J P, Han X G, Li P, Dong Z H, Wang X, Miao S M. J Manuf Sci Eng, 2009; 131: 031013[10] Zhu X P, Lei M K, Dong Z H, Ma T C. Rev Sci Instrum, 2003; 74 : 47[11] Zhang H T, Wang T M, Wang C, Wang W J, Han B X, Yan S, Zhao W J, Han Y F. Rare Met Mater Eng, 2003; 32: 216(张洪涛, 王天民, 王聪, 王文军, 韩宝玺, 颜莎, 赵渭江, 韩雅芳. 稀有金属材料工程, 2003; 32: 216)[12] Wang X, Zhang J S, Lei M K. Acta Metall Sin, 2007; 43: 393(王旭, 张俊善, 雷明凯. 金属学报, 2007; 43: 393)[13] Uglov V V, Anishchik V M, Astashynski V M, Cherenda N N, Gimro I G, Kovyazo A V. Surf Coat Technol, 2005; 200: 245[14] Gromilov S A, Kinelovskii S A, Kireenko I B. Combust, Explos Shock Waves, 2003; 39: 601[15] Zhu X P, Lei M K, Dong Z H, Miao S M, Ma T C. Surf Coat Technol, 2003; 173: 105[16] Jia K, Fischer T E. Wear, 1996; 200: 206[17] Satio H, Iwabuchi A, Shimizu T. Wear, 2004; 261: 126 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|