晶界网络特征对304不锈钢晶间应力腐蚀开裂的影响 |
胡长亮, 夏爽, 李慧, 刘廷光, 周邦新, 陈文觉 |
上海大学材料研究所, 上海 200072 |
|
EFFECT OF GRAIN BOUNDARY NETWORK ON THE INTERGRANULAR STRESS CORROSION CRACKING OF 304 STAINLESS STEEL |
HU Changliang, XIA Shuang, LI Hui, LIU Tingguang, ZHOU Bangxin, CHEN Wenjue |
Institute of Materials, Shanghai University, Shanghai 200072 |
引用本文:
胡长亮 夏爽 李慧 刘廷光 周邦新 陈文觉. 晶界网络特征对304不锈钢晶间应力腐蚀开裂的影响[J]. 金属学报, 2011, 47(7): 939-945.
.
EFFECT OF GRAIN BOUNDARY NETWORK ON THE INTERGRANULAR STRESS CORROSION CRACKING OF 304 STAINLESS STEEL[J]. Acta Metall Sin, 2011, 47(7): 939-945.
[1] Yang W D. Nuclear Reactor Materials Science. Beijing: Atomic Energy Press, 2000: 195(杨文斗. 反应堆材料学. 北京: 原子能出版社, 2000: 195)[2] Trillo E A, Murr L E. Acta Mater, 1999; 47: 235[3] Zhou Y, Aust K T, Erb U, Palumbo G. Scr Mater, 2001; 45: 49[4] Horn R M, Gordon G M, Ford F P, Cowan R L. Nucl Eng Des, 1997; 174: 313[5] Saito N, Tsuchiya Y, Kano F, Tanaka N. Corrosion, 2000; 56: 57[6] Watanable T. Res Mech, 1984; 11: 47[7] Kronberg M L, Wilson F H. Trans AIME, 1949; 185: 501[8] Randle V. Acta Mater, 2004; 52: 4067[9] Lehockey E M, Limoges D, Palumbo G, Sklarchuk J, Tomantscher K, Vincze A. J Power Sour, 1999; 78: 79[10] Thaveeprungsriporn V, Was G S. Metall Trans, 1997; 28: 2101[11] Lin P, Palumbo G, Erb U. Scr Metall Mater, 1995; 33: 1387[12] Shimada M, Kokawa H, Wang Z J, Sato Y S, Karibe I. Acta Mater, 2002; 50: 2331[13] Hu C L, Xia S, Li H, Liu T G, Zhou B X, Chen WJ, Wang N. Corros Sci, 2011; 53: 1880[14] Jin W Z, Yang S, Kokawa H, Wan Z J. J Mater Sci Technol, 2007; 23: 785[15] Rahimi S, Engelberg D L, Duff J A, Marrow T J. J Microsc, 2009; 233: 423[16] Brandon D G. Acta Mater, 1966; 14: 1479[17] Gerstman V Y, Bruemmer S M. Acta Mater, 2001; 49: 1589[18] Marrow T J, Babout L, Jivkor A P, Wood P, Engelberg D, Stevens N, Withers P J, Newman R C. J Nucl Mater, 2006; 352: 62[19] Xia S, Zhou B X, Chen W J, Wang W G. Scr Mater, 2006; 54: 2019[20] Xia S, Zhou B X, Chen W J. J Mater Sci, 2008; 43: 2990[21] Xia S, Zhou B X, Chen W J. Metall Mater Trans, 2009; 40A: 3016[22] Palumbo G, Aust K T, Lehockey E M, Erb U, Lin P. Scr Mater, 1998; 38: 1685[23] Arafin M A, Szpunar J A. Corr Sci, 2009; 51: 119[24] Arafin M A, Szpunar J A. Mater Sci Eng, 2009; A513–514: 254[25] Arafin M A, Szpunar J A. Comput Mater Sci, 2010; 47: 890[26] Pan Y, Adams B L, Olson T, Panayotou N. Acta Mater, 1996; 44: 4685[27] Alexandreanu B, Was G S. Scr Mater, 2006; 54: 1047 |
|