| 冷加工对含Mn铝合金管腐蚀行为的影响 |
| 王冠1,林晓群2 |
1.广东工业大学机电学院, 广州 510006
2.广东交通集团广东省公路建设有限公司, 广州 510600 |
|
| EFFECT OF COLD DEFORMATION ON THE CORROSION BEHAVIOUR OF Mn–CONTAINING ALUMINIUM ALLOY TUBE |
| WANG Guan1, LIN Xiaoqun2 |
1.Institute of Mechatronics, Guangdong University of Technology, Guangzhou 510006
2.Guangdong Road Construction Co. Ltd, Guangzhou 510600 |
引用本文:
王冠 林晓群. 冷加工对含Mn铝合金管腐蚀行为的影响[J]. 金属学报, 2011, 47(3): 361-366.
,
,
.
EFFECT OF COLD DEFORMATION ON THE CORROSION BEHAVIOUR OF Mn–CONTAINING ALUMINIUM ALLOY TUBE[J]. Acta Metall Sin, 2011, 47(3): 361-366.
| [1] Zamin M. Corrosion, 1981; 37: 627[2] Afseth A, Nordlien J H, Scamans G M, Nisancioglu K. Corros Sci, 2002; 44: 2543[3] Afseth A, Nordlien J H, Scamans G M, Nisancioglu K. Corros Sci, 2002; 44: 2491[4] Steven M. PhD Thesis, Delft University of Technology, 2002[5] Marshall G J, Bolingbroke R K, Gray A. Metall Mater Trans, 1993; 24A: 1935[6] Polmear I J. Light Alloys: Metallurgy of the Light Metals. Suffolk: St Edmundsbury Press Ltd., 1995: 24[7] Budgen N F. Aluminium and its Alloys. London: Pitman, 1947: 10[8] Wang G. PhD Thesis, University of Birmingham, 2007[9] Senkov O N, Fores F H, Stolyarov V V, Valiev R Z, Liu J. Nanostruct Mater, 1998; 10: 691[10] Ambat R, Davenport A J, Afseth A, Scamans G. J Electrochem Soc, 2004; 151: B53[11] Nisancioglu K. J Electrochem Soc, 1990; 137: 69[12] Afseth A, Nordlien J H, Scamans G M, Nisancioglu K. Corros Sci, 2001; 43: 2093[13] Afseth A, Nordlien J H, Scamans G M, Nisancioglu K. Corros Sci, 2002; 44: 145[14] Luiggi N J. Metall Mater Trans, 1997; 28B: 125[15] Luiggi N J. Z Metallkd, 1997; 88: 274[16] Luiggi N J. Metall Mater Trans, 1997; 28B: 149[17] Chen S P, Kuijpers N C W, Van Der Zwaag S. Mater Sci Eng, 2003; A341: 296[18] Nisancioglu K, Lunder O. Aluminium Alloys Physical and Mechanical Properties. Manchester: Engineering Materials Advisory Service Ltd., 1996: 1125 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|