| 轧制方向对Fe-3\%Si合金织构演变规律的影响 |
| 颜孟奇1), 杨平1), 蒋奇武2), 付勇军1,2), 毛卫民1) |
1) 北京科技大学 材料科学与工程学院, 北京 100083
2) 鞍钢股份有限公司冷轧硅钢厂, 鞍山 114021 |
|
| INFLUENCE OF ROLLING DIRECTION ON THE TEXTURE EVOLUTION OF Fe-3\%Si ALLOY |
| YAN Mengqi1), YANG Ping1), JIANG Qiwu2), FU Yongjun1,2), MAO Weimin1) |
1) School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
2) Anshan Steel Group, Cold Rolling Silicon Steel Division, Anshan 114021 |
引用本文:
颜孟奇 杨平 蒋奇武 付勇军 毛卫民. 轧制方向对Fe-3\%Si合金织构演变规律的影响[J]. 金属学报, 2011, 47(1): 25-33.
,
,
,
,
.
INFLUENCE OF ROLLING DIRECTION ON THE TEXTURE EVOLUTION OF Fe-3\%Si ALLOY[J]. Acta Metall Sin, 2011, 47(1): 25-33.
| [1] Dunn C G. Acta Metall, 1954; 2: 173[2] Hu H. Acta Metall, 1960; 8: 124[3] Misra S, Darmann C, Lucke K. Acta Metall, 1984; 32: 2185[4] Ushioda K, Hutchinson W B. ISIJ Int, 1989; 29: 862[5] Inokuti Y, Maeda C, Tanaka T. J Jpn Inst Met, 1985; 49: 417[6] Bottcher A, Hastenrath M, L¨ucke K. Texures Microstruct, 1991; 14–18: 799[7] Inokuti Y, Maeda C, Ito Y. Trans ISIJ, 1987; 27: 303[8] Shinozaki M, Matoba I, Kan T. Trans JIM, 1978; 19: 85[9] Inagaki H, Suda T. Texture, 1972; 1: 129[10] Dorner D, Zaefferer S, Lahn L, Raabe D. J Magn Magn Mater, 2006; 304: 183[11] Abe H, Matsuo M, Ito K. Trans JIM, 1986; 4: 28 |
|