| 冷却速率对变形与未变形X80管线钢组织的影响 |
| 邓伟,高秀华, 秦小梅, 高鑫, 赵德文, 杜林秀 |
| 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819 |
|
| EFFECT OF COOLING RATE ON MICROSTRUCTURE OF DEFORMED AND UNDEFORMED X80 PIPELINE STEELS |
| DENG Wei, GAO Xiuhua, QIN Xiaomei, GAO Xin, ZHAO Dewen, DU Linxiu |
| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819 |
引用本文:
邓伟 高秀华 秦小梅 高鑫 赵德文 杜林秀. 冷却速率对变形与未变形X80管线钢组织的影响[J]. 金属学报, 2010, 46(8): 959-966.
,
,
,
,
,
.
EFFECT OF COOLING RATE ON MICROSTRUCTURE OF DEFORMED AND UNDEFORMED X80 PIPELINE STEELS[J]. Acta Metall Sin, 2010, 46(8): 959-966.
| [1] Kim Y M, Kim S K, Lim Y J, Kim N J. ISIJ Int, 2002; 42: 1571
[2] Zhao M C, Shan Y Y, Xiao F R, Yang K, Li Y H. Mater Lett, 2002; 57: 141
[3] Bakkaloglu A. Mater Lett, 2002; 56: 200
[4] Zhao M C, Yang K, Shan Y Y. Mater Lett, 2003;57: 1496
[5] Zhao M C, Yang K, Xiao F R, Shan Y Y. Mater Sci Eng A,2003;355: 126
[6] Xiao F R, Liao B, Ren D L, Shan Y Y, Yang K. Mater Charact, 2005;54: 305
[7] Kim Y M, Lee H, Kim N J. Mater Sci Eng A, 2008;478: 361
[8] Pickering F B. Physical Metallurgy and Design of Steels. Essex: Applied Science Publishers Ltd., 1978: 64
[9] Dutta B, Valde′s E, Sellars C M. Acta Metall., 1992; 40 (4): 653
[10] Saito Y, Kimura M, Tanaska M, Sekine T, Tsubota K, Tanaka T. Kawasaki Steel Technical Report. 1984; 3: 12
[11] Aaronson H I, Enomoto M, Furuhara T, Reynolds W T. In: I. Tamura eds., Thermec 88, Int. Conf. on Physical Metallurgy of Thermomechanical Processing of Steels and Other Metals, Tokyo: Iron and Steel Institute of Japan. 1988; 1: 80
[12] Cotrina E, Iza-Mendia A, López , Gutiérrez I. Metall Mater Trans, 2004; A 35(1): 93
[13] Umemoto M, Guo Z H, Tamura I. Mater Sci Technol, 1987; 3: 249
[14] Honeycombe R W K. Steels Microstructures and Properties. London: Edward Arnold Pub. Ltd., 1980: 43
[15] Zhong Y, Xiao F R, Zhang J W. Acta Materialia, 2006; 54: 435
[16] Bhadeshia H K D H. Mater Sci Eng A, 1999; 273-275: 58
[17] Manabu T. Current Opinion in Solid State Mater Sci, 2004; 8: 213
[18] Liu Sh K, Yang L, Zhang J, Zhu D G. Acta Metall Sin, 1992; 28: A513
(刘世楷, 杨柳, 张筠, 朱德贵. 金属学报, 1992; 12: A513)
[19] Eghbali B, Abdollah-zadeh A. Scr Mater, 2006; 54: 1205
[20] Gregg J M, Bhadeshia H K D H. Metall Mater Trans, 1994; A 25:1603
[21] Quidort D, Bréchet Y. Scr Mater, 2002; 47: 151
[22] Li J, Sun F Y. Acta Metall Sin, 1990; 26: A 396
(李箭, 孙福玉.金属学报, 1990; 26: A396)
[23] Zhang B, Zhang H B. J Shanghai Jiaotong Uni, 2003; 37: 1522
(张斌, 张鸿冰.上海交通大学学报, 2003; 37: 1522)
[24] Bai D Q, Yue S, Maccagno T M, Jonas J J. Metall Mater Trans, 1998; A 29: 989
[25] Chang L C. Mater Sci Eng A, 2004; 368: 175
[26] Quidort D, Bréchet Y. ISIJ Int, 2002; 42: 1010
[27] Zhao J Z, Mesplont C , De Cooman B C. ISIJ Int, 2001; 41: 492
[28] Xu Z Y, Liu S K. Bainite Transformation and Bainite. Beijing: Science Press, 1991; 6: 179
(徐祖耀,刘世楷.贝氏体相变与贝氏体. 北京: 科学出版社,1991; 6: 179)
[29] Zhang W, Wu X C, Min Y A. Trans Mater Heat Treat, 2008; 29: 78
(张伟, 吴晓春, 闵永安. 材料热处理学报, 2008; 29: 78)
[30] Liu Z C, Ren H P. Diffusion Phase Transformation of Supercooled Austenite. Beijing: Science Press, 2007; 12: 88
(刘宗昌, 任慧平. 过冷奥氏体扩散型相变. 北京: 科学出版社, 2007; 12: 88)
[31] Cizek P, Wynne B P, Davies C H J, Muddle B C, Hodgson P D. Metall Mater Trans, 2002; A 33: 1331
[32] Hanzaki A Z, Pandi R, Hodgson P D, Yue S. Metall Mater Trans, 1993; A 24: 2657
[33] BAl D Q. S. Yue S, Maccagno T M, Jonas J J. ISIJ Int. 1998; 38: 371
[34] Bengochea R, Lo′Pez B, Gutierrez I. Metall Mater Trans, 1998; A 29: 417
[35] Fang H S. Bainite Transformation. Beijing: Science Press, 1999; 2: 59
(方鸿生. 贝氏体相变. 北京: 科学出版社, 1999; 2: 59)
[36] Bramfitt B L, Speer J G.. Metall Mater Trans, 1990; A 21: 817
[37] Yang Z G, Fang H S. Current Opinion in Solid State and Materials Science, 2005; 9: 277
[38] Singh S B, Bhadeshia H K D H. Mater Sci Eng, 1998; A245: 72
[39] Hwang B, Kim Y G, Lee S. Metall Mater Trans, 2005; 36A: 2107
[40] Díaz-Fuentes M, Madariga I, Gutiérrez I. Mater Sci Forum, 1998; 284–286: 245
[41] Rodríguez-Ibabe J M. Mater Sci Forum, 1998; 284–286: 51
[42] Diza-Fuentes M, Iza-Mendia A, Gutierrez I. Metall Mater Trans A, 2003; 34A: 2505
[43] Gourgues A F, Flower H M, Lindley T C. Mater Sci Technol, 2000; 16: 26
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|