P含量对Inconel 706合金凝固过程中(Laves+γ)共晶反应的影响
信昕1, 2), 黄爱华3), 祁峰2), 张伟红2), 刘芳2),  杨洪才1), 孙文儒2), 胡壮麒2)
1) 东北大学材料与冶金学院, 沈阳 110819
2) 中国科学院金属研究所, 沈阳 110016
3) 沈阳黎明发动机(集团)责任有限公司, 沈阳 110043
EFFECTS OF P CONTENT ON (LAVES+γ) EUTECTIC REACTION DURING INCONEL 706 ALLOY SOLIDIFICATION
XIN Xin1, 2), HUANG Aihua3), QI Feng2), ZHANG Weihong2),  LIU Fang2) ,YANG Hongcai1), SUN Wenru2) , HU Zhuangqi2)
1) School of Materials and Metallurgy, Northeastern University, Shenyang 110819
2) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
3) Shenyang Liming Aero--Engine Group Corporation, Shenyang 110043
引用本文:

信昕 黄爱华 祁峰 张伟红 刘芳 杨洪才 孙文儒 胡壮麒. P含量对Inconel 706合金凝固过程中(Laves+γ)共晶反应的影响[J]. 金属学报, 2010, 46(7): 873-878.
, , , , , , , . EFFECTS OF P CONTENT ON (LAVES+γ) EUTECTIC REACTION DURING INCONEL 706 ALLOY SOLIDIFICATION[J]. Acta Metall Sin, 2010, 46(7): 873-878.

全文: PDF(871 KB)  
摘要: 

研究了P对Inconel 706合金元素偏析和铸态组织的影响. 结果表明, P在合金凝固过程中显著地偏聚于剩余液相中, 并促进Nb和Ti等元素的偏聚, 从而促进富Nb的Laves相和富Ti的η-Ni3Ti相析出; 含0.004%P(质量分数)的Inconel 706合金枝晶间析出细小的(Laves+γ)共晶和少量针状η-Ni3Ti相; P含量超过0.016%以后, 枝晶间析出块状Laves相, Laves相颗粒之间析出大量密集的η-Ni3Ti板条; 此外, P含量由0.004%升高至0.016%, Laves相的初熔温度由1170-1180℃之间下降至1160-1170℃之间. 分析认为, 高度富集于剩余液相中的P强烈阻碍γ相的析出, 因此, P含量增加使合金的终凝温度降低, 而且导致合金的凝固结束反应由(Laves+γ)共晶转化为先析出富P的Laves相再析出γ基体的离异共晶反应.

关键词 : Inconel 706合金,  P含量,  凝固组织,  偏析    
Abstract:

The effects of P on elemental segregation and as-cast microstructure in Inconel 706 alloy were investigated in this paper. The results showed that P was markedly enriched in residual liquid and enhanced the segregation of Nb and Ti, which promoted the precipitation of Nb-enriched Laves phase and Ti-enriched η-Ni3Ti phase. In the as-cast alloy doped with 0.004% P (mass fraction), fine (Laves+γ) eutectic and needle like $\eta$ phase were formed in interdendritic region. As the P dopant was higher than 0.016%, blocky Laves phase was formed and lath η particles were precipitated among Laves particles. Moreover, with P increasing from 0.004\% to 0.016%, the incipient melting-point was found to drop from 1170-1180 ℃ to 1160-1170 ℃. In high P-doped alloys, the enrichment of P in the residual liquid was believed to hinder the solidification of γ phase, as a result, the final solidification temperature was found to be decreased and the solidification was terminated by the solidification of γ phase prior to the formation of P-bearing Laves phase rather than forming the (Laves+γ) eutectic.

Key words: Inconel 706 alloy    P content    solidified microstructure    segregation
收稿日期: 2010-01-09     
作者简介: 信 昕, 男, 1978年生, 博士生

[1] Schilke P W, Pepe J J, Schwant R C. In: Loria E A ed., Superalloys 718,625,706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1994: 1
[2] Schilke P W, Schwant R C. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 2001: 25
[3] Long Z D. Mater Rev, 1995; 5: 14
(龙正东. 材料导报, 1995; 5: 14)
[4] Hu Z Q, Sun W R, Guo S R, Lu D Z. Chin J Nonferrous Met, 2001; 11: 947
(胡壮麒, 孙文儒, 郭守仁, 卢德忠. 中国有色金属学报, 2001; 11: 947)
[5] Sun WR, Guo S R, Guo J T, Lu D Z, Hu Z Q. Acta Metall Sin, 1995; 31: 346
(孙文儒, 郭守仁, 郭建亭, 卢德忠, 胡壮麒. 金属学报, 1995; 31: 346)
[6] Sun WR, Guo S R, Lee J H, Park P K, Yoo Y S, choe S J, Hu Z Q. Mater Sci Eng, 1998; A247: 173
[7] Cao W D, Kennedy R L. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1994: 463
[8] Song H W. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 1999
(宋洪伟. 中国科学院金属研究所博士论文, 沈阳, 1999)
[9] Huang L F. PhD Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2007
(黄历锋. 中国科学院金属研究所博士论文, 沈阳, 2007)
[10] Yang S L. PhD Thesis, Northeastern University, Shenyang, 2006
(杨树林. 东北大学博士论文, 沈阳, 2006)
[11] Yang S L, Sun W R, Wang J X, Wang K L, Guo S R, Hu Z Q. Acta Metall Sin, 2009; 45: 815
(杨树林, 孙文儒, 王健熙, 王克亮, 郭守仁, 胡壮麒. 金属学报, 2009; 45: 815)
[12] Fesland J P, Petit P. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS– AIME, 1994: 229
[13] Meng X N, Sun W R, Guo S R, Lu D Z, Li N. Acta Metall Sin, 2004; 40: 613
(孟晓娜, 孙文儒, 郭守仁, 卢德忠, 李 娜. 金属学报, 2004; 40: 613)
[14] Chen C, Thompson R G, Davis S W. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale, PA: TMS–AIME, 1991: 81

[1] 马德新, 赵运兴, 徐维台, 王富. 重力对高温合金定向凝固组织的影响[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] 常松涛, 张芳, 沙玉辉, 左良. 偏析干预下体心立方金属再结晶织构竞争[J]. 金属学报, 2023, 59(8): 1065-1074.
[3] 刘继浩, 周健, 武会宾, 马党参, 徐辉霞, 马志俊. 喷射成形M3高速钢偏析成因及凝固机理[J]. 金属学报, 2023, 59(5): 599-610.
[4] 张利民, 李宁, 朱龙飞, 殷鹏飞, 王建元, 吴宏景. 交流电脉冲对过共晶Al-Si合金中初生Si相偏析的作用机制[J]. 金属学报, 2023, 59(12): 1624-1632.
[5] 陈学双, 黄兴民, 刘俊杰, 吕超, 张娟. 一种含富锰偏析带的热轧临界退火中锰钢的组织调控及强化机制[J]. 金属学报, 2023, 59(11): 1448-1456.
[6] 郭东伟, 郭坤辉, 张福利, 张飞, 曹江海, 侯自兵. 基于二次枝晶间距变化特征的连铸方坯CET位置判断新方法[J]. 金属学报, 2022, 58(6): 827-836.
[7] 吴国华, 童鑫, 蒋锐, 丁文江. 铸造Mg-RE合金晶粒细化行为研究现状与展望[J]. 金属学报, 2022, 58(4): 385-399.
[8] 李亚敏, 张瑶瑶, 赵旺, 周生睿, 刘洪军. Cu对Inconel 718合金Nb偏析影响机理的第一性原理研究[J]. 金属学报, 2022, 58(2): 241-249.
[9] 冯苗苗, 张红伟, 邵景霞, 李铁, 雷洪, 王强. 耦合热力学相变路径预测Fe-C包晶合金宏观偏析[J]. 金属学报, 2021, 57(8): 1057-1072.
[10] 曹江海, 侯自兵, 郭中傲, 郭东伟, 唐萍. 过热度对轴承钢凝固组织整体形貌特征及渗透率的影响[J]. 金属学报, 2021, 57(5): 586-594.
[11] 郭中傲, 彭治强, 柳前, 侯自兵. 高碳钢连铸坯大区域C元素分布不均匀度[J]. 金属学报, 2021, 57(12): 1595-1606.
[12] 张壮, 李海洋, 周蕾, 刘华松, 唐海燕, 张家泉. 齿轮钢铸态点状偏析及其在热轧棒材中的演变[J]. 金属学报, 2021, 57(10): 1281-1290.
[13] 郑秋菊, 叶中飞, 江鸿翔, 卢明, 张丽丽, 赵九洲. 微合金化元素La对亚共晶Al-Si合金凝固组织与力学性能的影响[J]. 金属学报, 2021, 57(1): 103-110.
[14] 张勇, 李鑫旭, 韦康, 韦建环, 王涛, 贾崇林, 李钊, 马宗青. 三联熔炼GH4169合金大规格铸锭与棒材元素偏析行为[J]. 金属学报, 2020, 56(8): 1123-1132.
[15] 李师居, 李洋, 陈建强, 李中豪, 许光明, 李勇, 王昭东, 王国栋. 电磁振荡场作用下双辊铸轧制备2099Al-Li合金的偏析行为及组织性能[J]. 金属学报, 2020, 56(6): 831-839.