金属学报  2010, Vol. 46 Issue (7): 850-856    DOI: 10.3724/SP.J.1037.2010.00036
  论文 本期目录 | 过刊浏览 |
退火过程Al-6Mg-0.7Mn-0.1Zr-0.3Er合金中纳米Al3(ZrxEr1-x)析出相的演化
宫博 文胜平 黄晖 聂祚仁
北京工业大学材料科学与工程学院, 北京 100124
EVOLUTION OF NANOSCALE Al3(ZrxEr1-x) PRECIPITATES IN Al-6Mg-0.7Mn-0.1Zr-0.3Er ALLOY ALLOY DURING ANNEALING
Gong Bo, WEN Shengping, HUANG Hui, NIE Zuoren
College of Materials Science and Engineering, Beijing University of Technology, Beijing 100124
引用本文:

宫博 文胜平 黄晖 聂祚仁. 退火过程Al-6Mg-0.7Mn-0.1Zr-0.3Er合金中纳米Al3(ZrxEr1-x)析出相的演化[J]. 金属学报, 2010, 46(7): 850-856.
, , , . EVOLUTION OF NANOSCALE Al3(ZrxEr1-x) PRECIPITATES IN Al-6Mg-0.7Mn-0.1Zr-0.3Er ALLOY ALLOY DURING ANNEALING[J]. Acta Metall Sin, 2010, 46(7): 850-856.

全文: PDF(910 KB)  
摘要: 

利用TEM对Al-6Mg-0.7Mn-0.1Zr-0.3Er合金在退火过程中Al3(ZrxEr1-x)的析出和生
长行为进行了研究. 结果表明: 低温退火(280℃, 470℃)和高温短时间退火(510℃, t≦100 h)
时, Al3(ZrxEr1-x)析出相的粗化符合LSW理论(n=1/3), 高温长时间退火(510℃, 300 h, 500 h)时,
Al3(ZrxEr1-x)析出相没有进一步粗化; Al3(ZrxEr1-x)析出相的粗化主要受Er, Zr等溶质原子在
$\alpha$-Al基体中的扩散影响. 二次析出相Al3(ZrxEr1-x)在较低温度(280和470℃)退火时均匀
分布于α-Al基体中, 较高温度(510℃)退火则呈线状不均匀分布. 在同一退火温度下, 随着
退火过程的进行, Al3(ZrxEr1-x)析出相的形貌逐渐从四方体向规则的球体过渡, 析出相
Al3(ZrxEr1-x)中的x增大.

关键词 : 退火,  Al$_{3}$(Zr$_{x}$Er$_{1-x}$),  粗化    
Abstract:

Erbium (Er) has attracted considerable attention as a substitute to scandium (Sc) for microalloying. The solid solution of Er and Zr decomposes to form a dispersion of secondary Al3(ZrxEr1-x) during annealing. This secondary Al3(ZrxEr1-x) precipitates improve strength, especially the elevated temperature strength. In the present paper we investigate the evolution of Al3(ZrxEr1-x) precipitate during annealing by transmission electron microscopy (TEM). The Al3(ZrxEr1-x) precipitates nucleate homogeneously at lower temperatures (280℃ and 470 ℃). The transition from homogeneous to heterogeneous nucleation at higher aging temperature (510℃) is a natural consequence of the reduced driving force for nucleus formation as the temperature increases and the Er supersaturation in the α-Al matrix decreases. The change in morphology of the Al3(ZrxEr1-x) precipitates from faceted to approximately spheroidal is associated with a change in the value of interfacial free energies. The diameter and the ratio of Zr/Er increase with increasing aging time at constant temperature. The coarsening of Al3(ZrxEr1-x) is dependent on the diffusivity of Er, Zr in α-Al.

Key words: annealing    Al3(ZrxEr1-x)    coarsening
收稿日期: 2010-01-19     
基金资助:

国家高技术研究发展计划项目2006AA03A207和2007AA03Z514资助

作者简介: 宫博, 男, 1984年生, 硕士生

[1] Hecht R, Kannan K, Ghosh A K, Bieler T R. Superplasticity and Superplastic Forming. Warredale, PA: TMS, 1995: 259
[2] Kaibyshev R, Musin F, Lesuer D R, Nieh T G. Mater Sci Eng, 2003; A342: 169
[3] Wang Z T, Tian R Z. Handbook of Aluminum Alloy and It’s Processing. Changsha: Central South University of Technology Press, 1989: 151
(王祝堂, 田荣璋. 铝合金及其加工手册. 长沙: 中南工业大学出版社. 1989: 151)
[4] Norman A F, Prangnell P B, Mcewen R S. Acta Mater, 1998; 46: 5715
[5] Filatov Yu A, Yelagin V I, Zakharov V V. Mater Sci Eng, 2000; A280: 97
[6] Lathabai S, Lloyd P G. Acta Mater, 2002; 50: 4275
[7] Jones M J, Humphreys F J. Acta Mater, 2003; 51: 2149
[8] Nie Z R, Jin T N, Fu J B, Xu G F, Yang J J, Zhou J. Mater Sci Forum, 2002; 396–402: 1731
[9] Nie Z R, Jin T N, Zou J X, Fu J B, Yang J J, Zuo T Y. Trans Nonferrous Met Soc China, 2003; 13: 509
[10] Yang J J, Nie Z R, Jin T N, Ruan H Q, Zuo T Y. Chin J Nonferrous Met, 2004; 14: 620
(杨军军, 聂祚仁, 金头男, 阮海琼, 左铁镛. 中国有色金属学报, 2004; 14: 620)
[11] Xu G F, Yang J J, Jin T N, Nie Z R, Yin Z M. Chin J Nonferrous Met, 2006; 16: 768
(徐国富, 杨军军, 金头男, 聂祚仁, 尹志民. 中国有色金属学报, 2006; 16: 768)
[12] Kendig K L, Miracle D B. Acta Mater, 2002; 50: 4165
[13] Marquies E A, Seidman D N. Acta Mater, 2001; 49: 1909
[14] Yin Z M, Jiang F, Pan Q L. Trans Nonferrous Met Soc China, 2003; 13: 515
[15] Karnesky R A, Dunand D C, Seidman D N. Acta Mater, 2009; 57: 4022
[16] van Dalen M E, Karnesky R A, Cabotaje J R, Dunand D C, Seidman D N. Acta Mater, 2009; 57: 4081
[17] Lin S P, Huang H, Wen S P, Nie Z R. Acta Metall Sin, 2009; 45: 978
(林双平, 黄 晖, 文胜平, 聂祚仁. 金属学报, 2009; 45: 978)
[18] Radmilovic V, Tolley A, Marquis E A, Rossell M D, Lee Z, Dahmen U. Scr Mater, 2008; 58: 529
[19] Wagner R, Kampmann R, Voorhees P. Homogeneous Second—Phase Precipitation, Phase Transformations in Materials. New York: Wiley–VCH, 2001: 309
[20] Thompson M E, Su C S, Voorhees P W. Acta Mater, 1994; 42: 2107
[21] Marquis E A, Seidman D N. Acta Mater, 2005; 53: 4259
[22] Fuller C B, Seidman D N. Acta Mater, 2005; 53: 5415
[23] Robson J D, Prangnell P B. Acta Mater, 2001; 49: 599

[1] 陈学双, 黄兴民, 刘俊杰, 吕超, 张娟. 一种含富锰偏析带的热轧临界退火中锰钢的组织调控及强化机制[J]. 金属学报, 2023, 59(11): 1448-1456.
[2] 金鑫焱, 储双杰, 彭俊, 胡广魁. 露点对连续退火0.2%C-1.5%Si-2.5%Mn高强钢选择性氧化及脱碳的影响[J]. 金属学报, 2023, 59(10): 1324-1334.
[3] 于少霞, 王麒, 邓想涛, 王昭东. GH3600镍基高温合金极薄带的制备及尺寸效应[J]. 金属学报, 2023, 59(10): 1365-1375.
[4] 杨平, 王金华, 马丹丹, 庞树芳, 崔凤娥. 成分对真空脱锰法相变控制高硅电工钢{100}织构的影响[J]. 金属学报, 2022, 58(10): 1261-1270.
[5] 王玉, 胡斌, 刘星毅, 张浩, 张灏云, 官志强, 罗海文. 退火温度对含Nb高锰钢力学和阻尼性能的影响[J]. 金属学报, 2021, 57(12): 1588-1594.
[6] 李索, 陈维奇, 胡龙, 邓德安. 加工硬化和退火软化效应对316不锈钢厚壁管-管对接接头残余应力计算精度的影响[J]. 金属学报, 2021, 57(12): 1653-1666.
[7] 姚小飞, 魏敬鹏, 吕煜坤, 李田野. (CoCrFeMnNi)97.02Mo2.98高熵合金σ相析出演变及力学性能[J]. 金属学报, 2020, 56(5): 769-775.
[8] 曹育菡,王理林,吴庆峰,何峰,张忠明,王志军. CoCrFeNiMo0.2高熵合金的不完全再结晶组织与力学性能[J]. 金属学报, 2020, 56(3): 333-339.
[9] 林晓冬,彭群家,韩恩厚,柯伟. 退火对热老化308L不锈钢焊材显微结构的影响[J]. 金属学报, 2019, 55(5): 555-565.
[10] 李文涛,王振玉,张栋,潘建国,柯培玲,汪爱英. 电弧复合磁控溅射结合热退火制备Ti2AlC涂层[J]. 金属学报, 2019, 55(5): 647-656.
[11] 刘后龙,马明玉,刘玲玲,魏亮亮,陈礼清. 热轧板退火工艺对19Cr2Mo1W铁素体不锈钢织构与成形性能的影响[J]. 金属学报, 2019, 55(5): 566-574.
[12] 邵成伟, 惠卫军, 张永健, 赵晓丽, 翁宇庆. 一种新型高强度高塑性冷轧中锰钢的组织和力学性能[J]. 金属学报, 2019, 55(2): 191-201.
[13] 邵毅, 李彦默, 刘晨曦, 严泽生, 刘永长. 低碳铁素体不锈钢高频直缝电阻焊管退火工艺优化[J]. 金属学报, 2019, 55(11): 1367-1378.
[14] 赵晓丽, 张永健, 邵成伟, 惠卫军, 董瀚. 两相区退火处理冷轧0.1C-5Mn中锰钢的氢脆敏感性[J]. 金属学报, 2018, 54(7): 1031-1041.
[15] 朱鸣芳, 邢丽科, 方辉, 张庆宇, 汤倩玉, 潘诗琰. 合金凝固枝晶粗化的研究进展[J]. 金属学报, 2018, 54(5): 789-800.