| 一维纳米材料导热性能的分子动力学模拟 |
| 高宇飞,孟庆元 |
| 哈尔滨工业大学航天学院, 哈尔滨 150001 |
|
| MOLECULAR DYNAMICS SIMULATION ON THERMAL CONDUCTIVITY OF ONE DIMENISON NANOMATERIALS |
| GAO Yufei, MENG Qingyuan |
| School of Astronautics, Harbin Institute of Technology, Harbin 150001 |
引用本文:
高宇飞 孟庆元. 一维纳米材料导热性能的分子动力学模拟[J]. 金属学报, 2010, 46(10): 1244-1249.
,
.
MOLECULAR DYNAMICS SIMULATION ON THERMAL CONDUCTIVITY OF ONE DIMENISON NANOMATERIALS[J]. Acta Metall Sin, 2010, 46(10): 1244-1249.
| [1] Mensah S Y, Allotey F K A, Nkrumah G, Mensah N G. Physica E,2004;23:152-158
[2] Chang C W, Han W Q, Zettl A. Appl Phys Lett, 2005,23(5):1883-1886
[3] Mingo N, Broido D A. Nano Lett,2005;5(7):1221-1225
[4] Hou Q W, Cao B Y, Guo Z Y. Journal of Engineering Thermophysics,2009;30(7):1207-1209[侯泉文,曹炳阳,过增元.工程热物理学报,2009;30(7):1207-1209]
[5] Pop E, Mann D, Wang Q, Goodson K, Dai H J. Nano Lett,2006;6(1):96-100
[6] Yu C, Shi L, Yao Z, Li D Y, Majumdar A. Nano Lett,2005;5(9):1842-1846
[7] Fujii M, Zhang X, Xie H Q, Ago H, Takahashi K, Ikuta T, Abe H, Shimizu T. Phys Rev Lett,2005;95(6):065502-1-4
[8] Kim P, Shi L, Majumdar A, Mceuen P L. Phys Rev Lett,2001;8721(21):215502-1-4
[9] Wang Z L, Tang D W, Li X B, Zheng X H, Zhang W G, Zheng L X, Zhu Y T, Jin A Z, Yang H F, Gu C Z. Appl Phys Lett,2007;91(12):123119-1-3
[10] Zhang G, Li B W. J Phys Chem B,2005;109(50):23823-23826
[11] Nanda J, Maranville C, Bollin S C, Sawall D, Ohtani H, Remillard J T, Ginder J M. J Phys Chem C,2008;112(3):654-658
[12] Mohammad A, Elena A, Michael C B, Florian M P. Nanotechnology,2009;20:115704-1-8
[13] Florian M P. J Chem Phys,1997;106(14):6082-6085
[14] Tersoff J. Phys Rev B,1988;37(12):6991-7000
[15] Karsten A, Wolfhard M. Comput Mater Sci,1998;10(1):111-115
[16] Hernandez E, Goze C, Bernier P, Rubio A. Phys Rev Lett,1998;80(20):4502-4505
[17] CAO B Y. Chinese Journal Of Computational Physics,2007;24(4):463-466[曹炳阳.计算物理,2007;24(4):463-466]
[18] Schelling P K, Phillpot S R, Keblinski P. Phys Rev B,2002;65(14): 144306-1-12
[19] Huang K. Solid Physics. Beijing:Higher Education Press,1988:145[黄昆著.固体物理学.北京:高等教育出版社,1988:145]
[20] Tian S G, Shen H J. Journal of Materials Science &Engineering,2009;27(2):213-215[田少岗,沈海军.材料科学与工程学报,2009;27(2):213-215]
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|