| 一种低碳钒微合金钢的动态再结晶与析出行为 |
| 陈礼清1, 赵阳1, 徐香秋2, 刘相华1 |
1. 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819
2. 中国第一汽车集团公司技术中心, 长春 130011 |
|
| DYNAMIC RECRYSTALLIZATION AND PRECIPITATION BEHAVIORS OF A KIND OF LOW CARBON V–MICROALLYED STEEL |
| CHEN Liqing 1, ZHAO Yang 1, XU Xiangqiu 2, LIU Xianghua 1 |
1. State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819
2. R & D Center, FAW Group Corporation, Changchun 130011 |
引用本文:
陈礼清 赵阳 徐香秋 刘相华. 一种低碳钒微合金钢的动态再结晶与析出行为[J]. 金属学报, 2010, 46(10): 1215-1222.
,
,
.
DYNAMIC RECRYSTALLIZATION AND PRECIPITATION BEHAVIORS OF A KIND OF LOW CARBON V–MICROALLYED STEEL[J]. Acta Metall Sin, 2010, 46(10): 1215-1222.
| [1] Poliak E I, Jonas J J. Acta mater, 1996; 44: 127
[2] Hansen S S, Vander Sande J B, Cohen M. Metall Mater Trans, 1980; 11A: 387
[3] Shanmugum S, Misra R D K, Mannering T, Panda D, Jansto S G. Mater Sci Eng, 2006; 437: 436
[4] Miyamoto G, Shinyoshi T, Yamaguchi J, Furuhara T, Maki T, Uemori U. Scr Mater, 2003; 48: 371
[5] Misra R D K, Weatherly G C, Hartmann J E, Boucek A J. Mater Sci Technol, 2001; 17: 1119
[6] Medina S F, Gomez M, Rancel L. Acta Mater, 2008; 58: 1000
[7] Medina S F, Hernandez C A. Acta Mater, 1996; 44: 165
[8] Ma L Q, Yuan X Q, Liu Z Y, Zhang P J, Jiao S H, Wu D, Wang G D. J Iron Steel Res, 2006; 18: 47
(马立强, 袁向前, 刘振宇, 焦四海, 吴 迪, 王国栋. 钢铁研究学报, 2006; 18: 47)
[9] Fernandez A I, Uranga P, Lopez B, Rodriguez-Ibabe J M. Mater Sci Eng, 2003; A361: 368
[10] Arribas M, Lopez B, Rodriguez-Ibabe J M. Mater Sci Eng, 2008; A485: 384
[11] Sellars C M, Tegart W J M. Mem Sci Rev Met, 1966; 63: 734
[12] Karhausen K, Kopp R. Metal working, 1992; 63: 253
[13] Medina S F, Hernandez C A. Acta Mater, 1996; 44: 142
[14] Cao J R, Liu Z D, Cheng S L, Yang G, Xie J X. Acta Metall Sin, 2007; 43: 37
(曹金荣, 刘正东, 程世长, 杨 钢, 谢建新. 金属学报, 2007; 43: 37)
[15] McQueen H J, Ryan N D. Mater Sci Eng, 2002; A322: 50
[16] Poliak E I, Jonas J J. ISIJ Int, 2003; 43: 686
[17] Akben M G, Weiss I, Jonas J J. Acta metall, 1981; 29: 114
[18] Lee K J. Scr Mater, 1999; 40: 840
[19] Tiitto K, Fitzsimons G, DeArdo A J. Acta metall, 1983; 31:1167
[20] Roberts W, Ahlblom B. Acta metall, 1978; 26
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|