Ni75AlxV25-x合金DO22到L12相变过程异相界面的结构及其迁移特征 |
张明义1;陈铮1;2;王永欣1;卢艳丽1;张静1;范晓丽1 |
1. 西北工业大学材料学院; 西安 710072
2. 西北工业大学凝固技术国家重点实验室; 西安 710072 |
|
STRUCTURE AND MIGRATION CHARACTERISTIC OF HETEROINTERFACES DURING THE PHASE TRANSFORMATION FROM DO22 TO L12 PHASE IN Ni75AlxV25−x ALLOYS |
ZHANG Mingyi 1; CHEN Zheng1;2; WANG Yongxin1; LU Yanli1; ZHANG Jing1; FAN Xiaoli 1 |
1. School of Materials Science and Engineering; Northwestern Polytechnical University; Xi'an 710072
2. State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
张明义 陈铮 王永欣 卢艳丽 张静 范晓丽. Ni75AlxV25-x合金DO22到L12相变过程异相界面的结构及其迁移特征[J]. 金属学报, 2009, 45(8): 930-936.
,
,
,
,
,
.
STRUCTURE AND MIGRATION CHARACTERISTIC OF HETEROINTERFACES DURING THE PHASE TRANSFORMATION FROM DO22 TO L12 PHASE IN Ni75AlxV25−x ALLOYS[J]. Acta Metall Sin, 2009, 45(8): 930-936.
[1] Massalki T B, Soffa W A, Laughlin D E. Metall Mater Trans, 2006; 37A: 825
[2] Wang S Q, Ye H Q. Curr Opin Solid State Mater, 2006; 10: 26
[3] Bos C, Sietsma J. Scr Mater, 2007; 57: 1085
[4] Bos C, Sommer F, Mittemeijer E J. Acta Mater, 2005; 53: 5333
[5] Singer H M, Singer I, Jacot A. Acta Mater, 2009; 57: 116
[6] Tateyama SShibuta Y, Suzuki TScr Mater, 2008; 59: 971
[7] Gong H R, Kong L T, Lai W S, Liu B X. Phys Rev, 2002; 66B: 104204
[8] Gong H R, Liu B X. Phys Rev, 2004; 70B: 134202
[9] Cahn J W, Mishin Y, Suzuki A. Acta Mater, 2006; 54: 4953
[10] Zhang M Y, Wang Y X, Chen Z, Zhang J, Zhao Y, Zhen H H. Acta Metall Sin, 2007, 43: 1101
(张明义, 王永欣, 陈铮, 张静, 赵彦, 甄辉辉. 金属学报, 2007; 43: 1101)
[11] Pareige C, Blavette D. Scr Mater, 2001; 44: 243
[12] Lu Y L, Chen Z, Wang Y X. Mater Lett, 2008; 62: 1385
[13] Li Y S, Chen Z, Lu Y L, Xu G D. Chin Phys, 2007; 16: 854
[14] Hou H, Zhao Y H, Zhao Y H. Mater Sci Eng, 2009; A499: 204
[15] Takeyama M, Kikuchi M. Intermetallics, 1998; 6: 573
[16] Khachaturyan A G. Theory of Structural Transformations in Solids. New York: Wiley, 1983: 1
[17] Poduri R, Chen L Q. Acta Mater, 1998; 46: 3915
[18] Poduri R, Chen L Q. Acta Mater, 1998; 46: 1719 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|