| 低碳钢中晶界铁素体/原奥氏体界面对贝氏体转变的影响 |
| 崔桂彬;郭晖;杨善武;贺信莱 |
| (北京科技大学材料科学与工程学院; 北京 100083) |
|
| INFLUENCE OF INTERFACE BETWEEN GRAIN BOUNDARY FERRITE AND PRIOR AUSTENITE ON BAINITE TRANSFORMATION IN A LOW CARBON STEEL |
| CUI Guibin; GUO Hui; YANG Shanwu; HE Xinlai |
| School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
崔桂彬 郭晖 杨善武 贺信莱. 低碳钢中晶界铁素体/原奥氏体界面对贝氏体转变的影响[J]. 金属学报, 2009, 45(6): 680-686.
,
,
,
.
INFLUENCE OF INTERFACE BETWEEN GRAIN BOUNDARY FERRITE AND PRIOR AUSTENITE ON BAINITE TRANSFORMATION IN A LOW CARBON STEEL[J]. Acta Metall Sin, 2009, 45(6): 680-686.
| [1] Ohmori Y, Ohtsubo H, Jung Y C, Okaguchi S, Ohtani H. Metall Mater Trans, 1994; 25A: 1981
[2] Furuhara T, Kawata H, Morito S, Miyamoto G, Maki T. Metall Mater Trans, 2008; 39A: 1003
[3] Babu S S, Bhadeshia H K D H. Mater Sci Eng, 1991; A142: 209
[4] Quidort D, Brechet Y J M. Acta Mater, 2001; 49: 4161
[5] Enomoto M, Aaronson H I. Metall Trans, 1987; 18A: 1547
[6] Purdy G R, Brechet Y J M. Acta Metall Mater, 1995; 43:3763
[7] Hillert M. Scr Mater, 2002; 46: 447
[8] Bradley J R, Rigsbee J M, Aaronson H I. Metall Trans, 1977; 8A: 323
[9] Bradley J R, Aaronson H I. Metall Trans, 1977; 8A: 317
[10] Tanaka T, Aaronson H I, EnomotoM. Metall Mater Trans,1995; 26A: 561
[11] Spanos G, Hall M G. Metall Mater Trans, 1996; 27A: 1517
[12] Hackenberg R E, Shiflet G J. Philos Mag, 2003; 83: 3367
[13] Hackenberg R E, Shiflet G J. Mater Charact, 2007; 58: 211
[14] Guo H, Purdy G R, Enomoto M, Aaronson H I. Metall Mater Trans, 2006; 37A: 1721
[15] Oi K, Lux C, Purdy G R. Acta Mater, 2000; 48: 2147
[16] Purdy G R. Acta Metall, 1978; 26: 477
[17] Menon E S K, Aaronson H I. Acta Metall, 1987; 35: 549
[18] Aaronson H I, Spanos G, Masamura R A, Vardiman R G,Moon DW, Menon E S K, Hall M G. Mater Sci Eng, 1995;B32: 107
[19] Guo H, Purdy G R. Metall Mater Trans, 2008; 39A: 950
[20] Zhang M X, Kelly P M. Scr Mater, 2002; 47: 749 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|