EBSD技术分析大晶粒NiAl合金高温塑性变形 组织演变与CSL特征晶界分布 |
胡静1;林栋樑2;王 燕1 |
1. 江苏工业学院材料科学与工程学院; 常州 213016
2. 上海交通大学材料科学与工程学院; 上海 200030 |
|
EBSD ANALYSES OF THE MICROSTRUCTURAL EVOLUTION AND CSL CHARACTERISTIC GRAIN BOUNDARY OF COARSE--GRAINED NiAl ALLOY DURING PLASTIC DEFORMATION |
HU Jing 1; LIN Dongliang2; WANG Yan1 |
1. School of Materials Science and Engineering; Jiangsu Polytechnic University; Changzhou 213016
2. School of Materials Science and Engineering; Shanghai Jiao Tong University; Shanghai 200030 |
引用本文:
胡静 林栋樑 王 燕. EBSD技术分析大晶粒NiAl合金高温塑性变形 组织演变与CSL特征晶界分布[J]. 金属学报, 2009, 45(6): 652-656.
,
,
.
EBSD ANALYSES OF THE MICROSTRUCTURAL EVOLUTION AND CSL CHARACTERISTIC GRAIN BOUNDARY OF COARSE--GRAINED NiAl ALLOY DURING PLASTIC DEFORMATION[J]. Acta Metall Sin, 2009, 45(6): 652-656.
[1] Li H T, Guo J T, Ye H Q. Rare Met Mater Eng, 2006; 35:1162
(李虎田, 郭建亭, 叶恒强. 稀有金属材料与工程, 2006; 35: 1162)
[2] Chokshi A H, Mukherjee A K, Langdon T G. Mater Sci Eng, 1993; R10: 237
[3] Mukherjee A K, Mishra R S. Mater Sci Forum, 1997; 243–245: 609
[4] Nieh T G, Wadsworth J. Mater Sci Eng, 1997; A239–240: 88
[5] Hu J, Lin D L. J Alloys Compd, 2006; 426: 162
[6] Hu J, Lin D L. Mater Sci Eng, 2006; A441: 142
[7] Jiang D M, Lin D L. Mater Lett, 2002; 57: 747
[8] Hu J, Lin D L. Mater Lett, 2004; 58: 1297
[9] Lin D L. Crystal Defects. Shanghai: Shanghai Jiao Tong University Press, 1996: 69
(林栋樑. 晶体缺陷. 上海: 上海交通大学出版社, 1996: 69)
[10] Zhang K, Wang W G, Fang X Y, Guo H. Acta Metall Sin,2008; 44: 652
(张坤, 王卫国, 方晓英, 郭 红. 金属学报, 2008; 44: 652)
[11] Watanabe T. Res Mech, 1984; 11: 47
[12] Wang W G, Zhou B X, Feng L, Zhang X, Xia S. Acta Metall Sin, 2006; 42: 715
(王卫国, 周邦新, 冯柳, 张欣, 夏爽. 金属学报, 2006; 42: 715)
[13] Cao S Q, Zhang J X, Wu J S, Chen J G. J Iron Steel Res,2005; 17: 51
(曹圣泉, 张津徐, 吴建生, 陈家光. 钢铁研究学报, 2005; 17: 51)
[14] Jiang D M, Ning J L, Sun J F, Hu Z M, Hou Y. Trans Nonferrous Met Soc China, 2008; 18: 248
[15] Jiang J, Godfrey A, Liu W, Liu Q. Mater Sci Eng, 2008; A483–484: 576
[16] Hu J. PhD Thesis, Shanghai Jiao Tong University, 2004
(胡静. 上海交通大学博士学位论文, 2004) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|