| 恒定磁场作用下Al-Pb合金快速定向凝固 |
| 赵九洲; 李海丽; 王青亮; 赵雷; 何杰 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| RAPID DIRECTIONAL SOLIDIFICATION OF Al-Pb ALLOY UNDER A STATIC MAGNETIC FIELD |
| ZHAO Jiuzhou; LI Haili; WANG Qingliang; ZHAO Lei; HE Jie |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
赵九洲 李海丽 王青亮 赵雷 何杰. 恒定磁场作用下Al-Pb合金快速定向凝固[J]. 金属学报, 2009, 45(11): 1344-1348.
,
,
,
,
.
RAPID DIRECTIONAL SOLIDIFICATION OF Al-Pb ALLOY UNDER A STATIC MAGNETIC FIELD[J]. Acta Metall Sin, 2009, 45(11): 1344-1348.
| [1] Zhao J Z, Ratke L. Z Metallkd, 1998; 89: 241
[2] Zhao J Z, Ratke L. Scr Mater, 1998; 39: 181
[3] Liu Y, Guo J J, Jia J, Su Y Q, Ding H S. Acta Metall Sin, 2001; 9: 917
(刘源, 郭景杰, 贾均, 苏彦庆, 丁宏升. 金属学报, 2001; 9: 917)
[4] Wang N, Wei B B. Mater Sci Eng, 2003; A345: 145
[5] Zhao J Z. Acta Metall Sin, 2002; 38: 525
(赵九洲. 金属学报, 2002; 38: 525)
[6] Zhao J Z, Ratke L, Jia J, Li Q C. J Mater Sci Technol, 2002; 18: 197
[7] Guo J J, Cui H B, Su Y Q, Bi W S, Jia J, Fu H Z. Spec Cast Nonferrous Alloys, 2004; 1: 1
(郭景杰, 崔红保, 苏彦庆, 毕维生, 贾 均, 傅恒志. 特种铸造及有色合金, 2004; 1: 1)
[8] Decarlo J L, Pirch R G. Metall Trans, 1984; 15A: 2155
[9] Foner S, Meniff E. Rev Sci Instr, 1968; 139: 171
[10] He J, Zhao J Z, Li H L, Zhang X F, Zhang Q X. Metall Mater Trans, 2008; 39A: 1174
[11] Zhang L, Wang E G, Zuo X W, He J C. Acta Metall Sin, 2008; 44: 165
(张林, 王恩刚, 左小伟, 赫冀成, 金属学报, 2008; 44: 165)
[12] Yasuda H, Ohnaka I, Fujimoto S. Mater Lett, 2004; 58: 911
[13] Yasuda H, Ohnaka I, Fujimoto S. Scr Mater, 2006; 54: 527
[14] Chester W. J Fluid Mech, 1957; 3: 304 |
|