Please wait a minute...
金属学报  2009, Vol. 45 Issue (1): 51-57    
  论文 本期目录 | 过刊浏览 |
2.25Cr-1Mo-0.25V钢焊缝中第二相高温回火转变
陶鹏1;张弛1;杨志刚1;武田裕之2
1 清华大学材料科学与工程系先进材料教育部重点实验室; 北京 100084 
2 (株)神户制钢所材料研究所材质制御研究室; 兵库651-2271; 日本
EVOLUTION OF SECOND PHASE IN 2.25Cr-1Mo-0.25V STEEL WELD METAL DURING HIGH TEMPERATURE TEMPERING
TAO Peng1; ZHANG Chi1; YANG Zhigang1;TAKEDA Hiroyuki2
1 Key Laboratory for Advanced Materials of Ministry of Education; Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 
2 Materials Design Section; Materials Research Laboratory; Kobe Steel Ltd.; Hyogo 651-2271; Japan
引用本文:

陶鹏 张弛 杨志刚 武田裕之. 2.25Cr-1Mo-0.25V钢焊缝中第二相高温回火转变[J]. 金属学报, 2009, 45(1): 51-57.
, , . EVOLUTION OF SECOND PHASE IN 2.25Cr-1Mo-0.25V STEEL WELD METAL DURING HIGH TEMPERATURE TEMPERING[J]. Acta Metall Sin, 2009, 45(1): 51-57.

全文: PDF(2146 KB)  
摘要: 

利用TEM和EDX技术, 研究了2.25Cr-1Mo-0.25V钢焊缝中第二相在700 ℃下保温一系列时间段的转变. 结果表明, 焊后空冷焊缝中的第二相为M3C, 回火过程中第二相主要组成为M3C+M7C3+M23C6. 长时间回火后M3C发生球化并消失, 初期析出的低wCr/wFe(Cr与Fe的质量比)的M7C3是亚稳相, M23C6只能在较低的回火参数范围内存在, 后期形成了wCrwFe更高的M7C3稳定的第二相. M3C多呈球状,M7C3和M23C6多为长条状和块状.

关键词 : 焊缝,  第二相,  碳化物,  回火,  低合金钢2.25Cr--1Mo--0.25V    
Abstract:

The evolution of the second phase in 2.25Cr–1Mo–0.25V steel weld metal during holding at 700 ℃ for a series of durations was studied by TEM and EDX. The precipitates in the as– welded specimen are M3C carbides, and during tempering M7C3 and M23C6 carbides appeared. After long term tempering M3C carbides spheroidized and disappeared. In the early tempering stage M7C3 carbide with low wCr/wFe is metastable phase. M23C6 carbide can exist only under low tempering parameter, and M7C3 carbide with high wCr/wFe formed in the late stage is the stable phase. M3C carbides are often sphere–liked, M7C3 and M23C6 carbides are rod–shaped and lump–shaped.

Key words: weld metal    second phase    carbide    tempering    low alloy steel 2.25Cr--1Mo--0.25V
收稿日期: 2008-06-04     
ZTFLH: 

TG146.1

 
作者简介: 陶鹏, 男, 1985年生, 硕士生

[1] Bhadeshia H K D H. Bainite in Steels. 2nd Ed., London: The Institute of Materials, 2001: 323
[2] Davis J R. Metals Handbook. Vol.1, 10th Ed., Materials Park, OH: ASM International, 1990: 617
[3] Klueh R L, Swindeman R W. Metall Trans, 1986; 17A: 1027
[4] Miranda R M, Fortes M A. Mater Sci Eng, 1989; A108: 1
[5] Cheruvu N S. Metall Trans, 1989; 20A: 87
[6] Thomson R C, Badeshia H. Mater Sci Technol, 1994; 10: 193
[7] Fujita N, Bhadeshia H K D H. ISIJ Int, 2002; 42: 760
[8] Baker R G, Nutting J. J Iron Steel Inst, 1959; 192: 257
[9] Tsai M C, Chiou C S, Yang J R. J Mater Sci, 2003; 38: 2373
[10] Tsai M C, Yang J R. Mater Sci Eng, 2003; A340: 15
[11] Janovec J, Svoboda M, Kroupa A, Vyrostkova A. J Mater Sci, 2006; 41: 3425
[12] Sourmail T. Mater Sci Technol, 2001; 17: 1
[13] Inouoe A, Masumoto T. Metall Trans, 1980; 11A: 739
[14] Lane J R, Grant N J. Trans ASM, 1952; 44: 113
[15] Sims C T. J Met, 1969; 21: 27
[16] V´yrostkov´a A, Kroupa A, Janovec J, Janovec J. Acta Mater, 1998; 46: 31
[17] Kroupa A, V´yrostkov´a A, Svoboda M, Janovec J. Acta Mater, 1998; 46: 39
[18] Janovec J, Svoboda M, Vyrostkova A, Kroupa A. Mater Sci Eng, 2005; A402: 288

[1] 刘继浩, 周健, 武会宾, 马党参, 徐辉霞, 马志俊. 喷射成形M3高速钢偏析成因及凝固机理[J]. 金属学报, 2023, 59(5): 599-610.
[2] 娄峰, 刘轲, 刘金学, 董含武, 李淑波, 杜文博. 轧制态Mg-xZn-0.5Er合金板材组织及室温成形性能[J]. 金属学报, 2023, 59(11): 1439-1447.
[3] 李闪闪, 陈云, 巩桐兆, 陈星秋, 傅排先, 李殿中. 冷速对高碳铬轴承钢液析碳化物凝固析出机制的影响[J]. 金属学报, 2022, 58(8): 1024-1034.
[4] 沈国慧, 胡斌, 杨占兵, 罗海文. 回火温度对含 δ 铁素体高铝中锰钢力学性能和显微组织的影响[J]. 金属学报, 2022, 58(2): 165-174.
[5] 周成, 赵坦, 叶其斌, 田勇, 王昭东, 高秀华. 回火温度对1000 MPa级NiCrMoV低碳合金钢微观组织和低温韧性的影响[J]. 金属学报, 2022, 58(12): 1557-1569.
[6] 骆文泽, 胡龙, 邓德安. SUS316不锈钢马鞍形管-管接头的残余应力数值模拟及高效计算方法开发[J]. 金属学报, 2022, 58(10): 1334-1348.
[7] 王占花, 惠卫军, 谢志奇, 张永健, 赵晓丽. 回火对钒钛微合金化Mn-Cr系贝氏体型非调质钢组织和性能的影响[J]. 金属学报, 2020, 56(11): 1441-1451.
[8] 武华健, 程仁山, 李景仁, 谢东升, 宋锴, 潘虎成, 秦高梧. Al含量对Mg-Sn-Ca合金微观组织与力学性能的影响[J]. 金属学报, 2020, 56(10): 1423-1432.
[9] 杨柯,梁烨,严伟,单以银. (9~12)%Cr马氏体耐热钢中微量B元素的择优分布行为及其对微观组织与力学性能的影响[J]. 金属学报, 2020, 56(1): 53-65.
[10] 李嘉荣,谢洪吉,韩梅,刘世忠. 第二代单晶高温合金高周疲劳行为研究[J]. 金属学报, 2019, 55(9): 1195-1203.
[11] 董福涛,薛飞,田亚强,陈连生,杜林秀,刘相华. 退火温度对TWIP钢组织性能和氢致脆性的影响[J]. 金属学报, 2019, 55(6): 792-800.
[12] 冯汉臣,闵学刚,魏大圣,周立初,崔世云,方峰. 低温回火对超大形变冷拔珠光体钢丝显微组织和力学性能的影响[J]. 金属学报, 2019, 55(5): 585-592.
[13] 黄宇, 成国光, 李世健, 代卫星. Ce微合金化H13钢中一次碳化物的析出机理及热稳定性研究[J]. 金属学报, 2019, 55(12): 1487-1494.
[14] 曾荣昌, 崔蓝月, 柯伟. 医用镁合金:成分、组织及腐蚀[J]. 金属学报, 2018, 54(9): 1215-1235.
[15] 刘金辉, 宋影伟, 单大勇, 韩恩厚. 铸态和锻造态Mg-5Y-7Gd-1Nd-0.5Zr合金腐蚀行为对比研究[J]. 金属学报, 2018, 54(8): 1141-1149.