| 压铸过程中铸件-铸型界面换热系数与铸件凝固速率的关系 |
| 郭志鹏1 ; 熊守美1; Mei Li2 ; John Allison2 |
1 清华大学机械工程系先进成形制造教育部重点实验室;北京 100084
2 Research & Advanced Engineering Department; Scientific Research Laboratory; Ford Motor Company; Dearborn; MI 48121; USA |
|
| RELATIONSHIP BETWEEN METAL-DIE INTERFACIAL HEAT TRANSFER COEFFICIENT AND CASTING SOLIDIFICATION RATE IN HIGH PRESSURE DIE CASTING PROCESS |
| GUO Zhipeng1; XIONG Shoumei1; Mei Li2;John Allison2 |
1 Key Laboratory for Advanced Materials Processing Technology; Ministry of Education; Department of Mechanical Engineering; Tsinghua University; Beijing 100084
2 Research & Advanced Engineering Department; Scientific Research Laboratory; Ford Motor Company; Dearborn; MI 48121; USA |
引用本文:
郭志鹏 熊守美 Mei Li John Allison. 压铸过程中铸件-铸型界面换热系数与铸件凝固速率的关系[J]. 金属学报, 2009, 45(1): 102-106.
,
,
,
.
RELATIONSHIP BETWEEN METAL-DIE INTERFACIAL HEAT TRANSFER COEFFICIENT AND CASTING SOLIDIFICATION RATE IN HIGH PRESSURE DIE CASTING PROCESS[J]. Acta Metall Sin, 2009, 45(1): 102-106.
| [1] Pehlke R D, Berry J T. In: ASM International, ed., Advances in Aluminum Casting Technology II, Materials Park, OH: ASM International, 2002: 177
[2] Hallam C P, Griffiths W D. Metall Mater Trans, 2004; 35B: 721
[3] Dour G, Dargusch M, Davidson C, Nef A. J Mater Process Technol, 2005; 169: 223
[4] Hamasaiid A, Dargusch M S, Davidson C J, Tovar S, Loulou T, Rezai–Aria F, Dour G. Metall Mater Trans, 2007; 38A: 1303
[5] Guo Z P, Xiong S M, Cho S–H, Choi J–K. Acta Metall Sin, 2007; 43: 1155
(郭志鹏, 熊守美, 尚铉, 崔正吉.金属学报, 2007; 43: 1155)
[6] Guo Z P, Xiong S M, Cho S–H , Choi J–K. Acta Metall Sin, 2007; 43: 1149)
(郭志鹏, 熊守美, CAO尚铉, 崔正吉.金属学报, 2007; 43: 1149)
[7] Guo Z P, Xiong S M, Cho S–H , Choi J–K. Acta Metall Sin, 2008; 44: 433)
(郭志鹏, 熊守美, CAO尚铉, 崔正吉.金属学报, 2008; 44: 433)
[8] Nelson C W. In: SDCE (the Society of Die Casting Engineers), ed., 6th SDCE International Die Casting Congress, Cleveland, OH: SDCE, 1970: 1
[9] Hong S, Backman D G, Mehrabian R. Metall Mater Trans, 1979; 10B: 299
[10] Papai J, Mobley C. In: NADCA (North American Die Casting Association), ed., Transactions of the NADCA Congress, Detroit, MI: NADCA, 1991: 377
[11] Hamasaiid A, Dour G, Dargusch M, Loulou T, Davidson C, Savage G. In: Gandin C–A, Bellet M, eds., Modeling of Casting, Welding and Advanced Solidification Processes–XI, Warrendale, PA: Minerals, Metals and Materials Society, 2006: 1205
[12] Guo Z P, Xiong S M, Cho S–H, Choi J–K. Acta Metall Sin, 2007; 43: 607
(郭志鹏, 熊守美, CAO尚铉, 崔正吉.金属学报,2007; 43: 607) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|