| 新型低碳贝氏体钢在含氯离子环境中的腐蚀行为和表观力学性能的变化 |
| 王树涛;杨善武;高克玮;沈晓安;贺信莱 |
| 北京科技大学材料物理与化学系 |
|
| CORROSION BEHAVIOR AND VARIATION OF APPARENT MECHANICAL PROPERTY OF ONE NEWLY-DEVELOPED LOW CARBON BAINITIC STEEL IN ENVIRONMENT CONTAINING CHLORIDE ION |
| Shu-Tao WANG;;Kewei GAO;; |
| 北京科技大学 |
引用本文:
王树涛; 杨善武; 高克玮; 沈晓安; 贺信莱 . 新型低碳贝氏体钢在含氯离子环境中的腐蚀行为和表观力学性能的变化[J]. 金属学报, 2008, 44(9): 1116-1124 .
,
,
,
,
.
CORROSION BEHAVIOR AND VARIATION OF APPARENT MECHANICAL PROPERTY OF ONE NEWLY-DEVELOPED LOW CARBON BAINITIC STEEL IN ENVIRONMENT CONTAINING CHLORIDE ION[J]. Acta Metall Sin, 2008, 44(9): 1116-1124 .
[1]Yang D J,Shen Z S.Metal Corrosion.2nd Ed.,Beijing: Metallurgical Industry Press,1999:216 (杨德钧,沈卓身.金属腐蚀学.第2版,北京:冶金工业出版社,1999:216) [2]General Administration of Quality Supervision,Inspection and Quarantine of the People's Republic of China.GB/T 4171 2000,Beijing:Standards Press of China,2000 (国家技术监督局.GB/T4171-2000,北京:中国标准出版社,2000) [3]Wang X M,Shang C J,Yang S W,He X L.Acta Metall Sin,2002;38:661 (王学敏,尚成嘉,杨善武,贺信莱.金属学报,2002:38:661) [4]Shang C J,Wang X M,Yang S W,He X L,Wu H B.Acta Metall Sin,2003;39:1019 (尚成嘉,王学敏.杨善武,贺信莱,武会宾.金属学报,2003;39:1019) [5]Weng Y Q.The Ultra-Fine Crystal Steel.Beijing:Metal- lurgical Industry Press,2003:279 (翁宇庆.超细晶钢.北京:冶金工业出版社,2003:279) [6]Zhao Z Y.The Design of Alloy Steel.Beijing:National Defence Industry Press,1999:106 (赵振业.合金钢设计.北京:国防工业出版社,1999:106) [7]The American Society for Testing and Materials.ASTM G 44-99,1999 [8]The American Society for Testing and Materials.ASTM E 8M-03,2003 [9]Chen Y Y,Tzeng H J,Wei L I,Wang L H,Oung J C, Shih H C.Corros Sci,2005;47:1001 [10]Kamimura T,Hara S,Miyuki H,Yamashita M,Uchida H. Corros Sci,2006;48:2799 [11]Nishimura T,Katayama H,Noda K,Kodama T.Corro- sion,2000;56:935 [12]Bousselmi L,Fiaud C,Tribollet B,Triki E.Corros Sci, 1997;39:1711 [13]Bousselmi L,Fiaud C,Tribollet B,Trim E.Electrochim Acta,1999;44:4357 [14]Santana Rodrfguez J J,Santana Hernández F J,González J E.Corros Sci,2002;44:2597 [15]The General Edit Committee of the Steel Material Hand- book.The Steel Material Handbook,Vol.2:Low Alloy High Strength Steel.Beijing:Standards Press of China, 2003:32 (《钢铁材料手册》总编辑委员会.钢铁材料手册,第2卷:低合金高强度钢.北京:中国标准出版社,2003:32) [16]Huang J Z,Zuo Y.Material Corrosion Resistance and Corrosion Data.Beijing:Chemical Industry Press,2003: 84 (黄建中,左禹.材料耐蚀性和腐蚀数据.北京:化学工业出版社,2003:84) [17]Chen X H,Dong J H,Han E H,Ke W.Mater Lett,2007; 61:4050 [18]Xu N X,Zhao L Y,Ding C H,Zhang C D,Li R S,Zhong Q D.Corros Sci,2002;44:163 [19]Li B,Weng Y J,Li X Y.Electrochern Commun,2005;7: 1033 [20]ZhangQC,WuJS,WangJ J,Zheng W L,Chen J G,Li A B.Mater Chern Phys,2002;77:603 [21]Yamashita M,Miyuki H,Mastsuda Y,Nagano H,Misawa T.Corros Sci,1994;36:283 [22]Mizoguchi T,Ishii Y,Okada T,Kimura M,Kihira H.Cot- ros Sci,2005;47:2477 [23]Yang D J,Shen Z S.Metal Corrosion.2nd Ed.,Beijing: Metallurgical Industry Press,1999:293 (杨德钧,沈卓身金属腐蚀学.第2版,北京:冶金工业出版社,1999:293) [24]Yu F Z.Corrosion Resistance of Metal Materials.Beijing: Science Press,1982:21 (于福洲.金属材料的耐腐蚀性.北京:科学出版社,1982:21) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|