| 熔体流动对Mg-H共晶二维定向凝固的影响 |
| 王雪;李言祥;刘源 |
| 清华大学机械工程系先进成形制造教育部重点实验室 |
|
| Effect of Transverse Convection Induced by Density Differences on Bidirectional Solidification of Metal-Gas Eutectic |
| ;; |
| 清华大学机械工程系 |
引用本文:
王雪; 李言祥; 刘源 . 熔体流动对Mg-H共晶二维定向凝固的影响[J]. 金属学报, 2008, 44(9): 1057-1062 .
[1]Shapovalov V I.US Pat,No.5,181,549,1993 [2]Banhart J.Prog Mater Sci,2001;46:559 [3]Nakajima H.Prog Mater Sci,2007;52:1091 [4]Zheng Y.Master Thesis,MIT,Cambridge,MA,1995 [5]Zhang H W.Doctoral Dissertation,Tsinghua University, Beijing,2006 (张华伟.清华大学博士学位论文,北京,2006) [6]Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2006;42: 1165 (张华伟,李言祥,刘源.金属学报,2006;42:1165) [7]Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2006;42: 1171 (张华伟,李言祥,刘源.金属学报,2006;42:1171) [8]Wang X,Li Y X,Liu Y.Acta Metall Sin,2006;42:1075 (王雪,李言祥,刘源.金属学报,2006;42:1075) [9]Wang X,Li Y X,Liu Y.Acta Metall Sin,2007;43:6 (王雪,李言祥,刘源.金属学报,2007;43:6) [10]Wang X,Li Y X,Liu Y.Mater Sci Eng,2007;A444:306 [11]Shapovalov V I.Mater Sci Forum,2007;539-543:1183 [12]Liu Y,Li Y X.Scr Mater,2003;49:379 [13]Shapovalov V I.Adv Eng Mater,2004;6:407 [14]Shapovalov V I.USSR Pat,No.3,032,290,1981 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|