| 退火温度对双相纤维复合Cu-12%Ag合金织构的影响 |
| 贺佳;孟亮 |
| 浙江大学金属材料研究所 |
|
| EFFECTS OF ANNEALING TEMPERATURE ON INTENSITY AND DISTRIBUTION OF CRYSTAL TEXTURE IN Cu-12% Ag FILAMENTARY COMPOSITE |
| Liang Meng; |
| 浙江大学金属材料研究所 |
引用本文:
贺佳; 孟亮 . 退火温度对双相纤维复合Cu-12%Ag合金织构的影响[J]. 金属学报, 2008, 44(1): 43-48 .
,
.
EFFECTS OF ANNEALING TEMPERATURE ON INTENSITY AND DISTRIBUTION OF CRYSTAL TEXTURE IN Cu-12% Ag FILAMENTARY COMPOSITE[J]. Acta Metall Sin, 2008, 44(1): 43-48 .
[1]Zhang L,Yan F,Meng L.Mater Rev,2003;17(5):15 (张雷,颜芳,孟亮.材料导报,2003;17(5):15) [2]Benghalem A,Morris D G.Acta Mater,1997;45:397 [3]Maeda H,Inoue K,Kiyoshi T,Asano T,Sakai Y,Takeuchi T.Physica,1996;216B:141 [4]Freudenberger J,Kozlova N,Gaganov A,Schultz L,Witte H,Jones H.Cryogenics,2006;46:724 [5]Grünberger W,Heilmaier M,Schultz L.Physica,2001; 643B:294 [6]Ohsaki S,Yamazaki K,Hono K.Scr Mater,2003;48:1569 [7]Sakai Y,Schneider-Muntau H J.Acta Mater,1997;45: 1017 [8]Han K,Vasquez A A,Xin Y,Kalu P N.Acta Mater,2003; 51:767 [9]He J,Liu J B,Meng L.Acta Metall Sin,2007;43:643 (贺佳,刘嘉斌,孟亮.金属学报,2007;43:643) [10]Hong S I,Hill M A.Acta Mater,1998;46:4111 [11]Hong S I,Hill M A.Mater Sci Eng,1999;A264:151 [12]Kwon H J,Hong S I.J Alloys Compd,2001;32:161 [13]Yan F,Meng L,Zhang L.Acta Metall Sin,2004;40:891 (颜芳,孟亮,张雷.金属学报,2004;40:891) [14]Yang J X.Physical Foundation of Metals Plastic Defor- mation.Beijing:Metallurgical Industry Press,1988:248 (杨觉先.金属塑性变形物理基础.北京:冶金工业出版社,1988:248) [15]Zhang X Y.Crystal Texture of Metals and Alloys.Beijing: Science Press,1976:79 (张信钰.金属和合金的织构.北京:科学出版社,1976:79)V |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|