| AZ31B镁合金挤压管材的内高压成形性能 |
| 何祝斌;王小松;苑世剑;许爱军 |
| 哈尔滨工业大学 |
|
| EXPERIMENTAL RESEARCH INTO THE FORMABILITY OF AZ31B EXTRUDED TUBE |
| Zhu-Bin He; |
| 哈尔滨工业大学 |
引用本文:
何祝斌; 王小松; 苑世剑; 许爱军 . AZ31B镁合金挤压管材的内高压成形性能[J]. 金属学报, 2007, 43(5): 534-538 .
,
,
,
.
EXPERIMENTAL RESEARCH INTO THE FORMABILITY OF AZ31B EXTRUDED TUBE[J]. Acta Metall Sin, 2007, 43(5): 534-538 .
[1] Merklein M, Geiger M. J Mater Process Technol, 2002; 125-126: 532 [2] Novotny S, Geiger M. J Mater Process Technol, 2003; 138: 594 [3] Imaninejad M, Subbash G, Loukus A. J Mater Process Technol, 2004; 147: 247 [4] Groche P, Breitenbach G. In: Siegert K, ed., Proc Hydro-forming of Tubes, Extrusions and Sheet Metals, Frankfult: MAT Information, 2005: 219 [5] Banabic D. Formability of Metallic Materials, Plastic Anisotropy, Formability Testing and Forming Limits. Berlin: Springer, 2000: 92 [6] Sokolowski T, Gerke K, Ahmetoglu M, Altan T. J Mater Process Technol, 2000; 98: 34 [7] Huang Y M, Yang M T. J Key Eng Mater, 2003; 233-236: 311 [8] Huang Y M. In: Manabe K, ed., Proc Tubehydro, Nagoya, Japan: Sigma Publishing, 2003: 105 [9] Huang J C. Dissertation for the Doctor Degree, National Sun Yat-Sen University, Taibei, 2004 (黄建超.国立中山大学材料科学研究所博士学位论文,台北, 2004) [10] Wu S C. Superplastic Deformation Theory of Metals. Beijing: National Defense Industry Press, 1997: 18 (吴诗惇.金属超塑性变形理论.北京;国防工业出版社,1997: 18) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|