| 深过冷Cu--20%Pb亚偏晶合金凝固组织的细化机制 |
| 刘丽琴 张忠明 徐春杰 郭学锋 |
| 西安理工大学材料科学与工程学院 |
|
| Refinement Mechanism of the Solidification Structure of Cu--20%Pb Hypomonotectic Alloy by Deeply Undercooled Treatment |
| LIU Liqin; ZHANG Zhongming; XU Chunjie; GUO Xuefeng |
| School of Materials Science and Engineering; Xi'an University of Technology |
引用本文:
刘丽琴; 张忠明; 徐春杰; 郭学锋 . 深过冷Cu--20%Pb亚偏晶合金凝固组织的细化机制[J]. 金属学报, 2007, 43(11): 1138-1144 .
,
,
,
.
Refinement Mechanism of the Solidification Structure of Cu--20%Pb Hypomonotectic Alloy by Deeply Undercooled Treatment[J]. Acta Metall Sin, 2007, 43(11): 1138-1144 .
[1]Yang G C,Xie H,Hao W X.Trans Nonferrous Met Soc Chin,2006;16:290 [2]Hao W X,Yang G C,Xie H.Foundry Technol,2004;25: 105 (郝维新,杨根仓,谢辉.铸造技术,2004;25:105) [3]Sun W L,Zhang Z M,Xu C J,Guo X F.Trans Mater Heat Treat,2005;26(6):53 (孙万里,张忠明,徐春杰,郭学锋.材料热处理学报,2005;26(6):53) [4]Zhang Z M,Sun W L,Xu C J,Guo X F.J Xi'an Univ Technol,2005;21:118 (张忠明,孙万里,徐春杰,郭学锋.西安理工大学学报,2005;21:118) [5]Sun W L,Zhang Z M,Xu C J,Guo X F.Ordnance Mater Sci Eng,2005;28(1):66 (孙万里,张忠明,徐春杰,郭学锋.兵器材料科学与工程,2005;28(1):66) [6]Zheng H X,Li J G,Guo X F.Mater Design,2007;28: 558 [7]Boettinger W J,Coriell S R,Trivedi R.Rapid Solidifi- cation Processing:Principle and Technologes IV.In: Mehrabian R,Parrish P A,eds.,Baton Rouge:Claitor's Publishing Division,1988:13 [8]Trivedi R,Lipton J,Kurz W.Acta Metall,1987;35:965 [9]Kurz W,Trivedi R.Acta Metall Mater,1990;38:1 [10]Aziz M J.J Appl Phys,1982;53:1158 [11]Guo X F,Liu F,Yang G C,Xing J D.Acta Metall Sin, 2000;36:352 (郭学锋,刘峰,杨根仓,邢建东.金属学报,2000;36:352) [12]Fan J F,Yang G C,Liu X B,Wang J C,Song G S.J Nonferrous Met Chin,2003;13:344 (樊建锋,杨根仓,刘新宝,王锦程,宋广生.中国有色金属学报,2003;13:344) [13]Guo X F,Liu F,Yang G C,Xing J D.Prog Nat Sci,2000; 10:734 (郭学锋,刘峰,杨根仓,邢建东.自然科学进展,2000;10:734) [14]Eric A B.Smithells Metals Reference Book.6ed.London: Robert Hartholl Ltd,1983:8 [15]Eckler K,Cochrane R F,D M Herlach,Jurisch M.Phys Rev,1992;45B:5019 [16]Eckler K,Herlach D M,Aziz M J.Acta Metall Mater, 1994;42:975 |
|