| 应变梯度塑性理论模拟晶粒尺寸对铝多晶体强度的影响 |
| 周 丽 李守新 柯 伟 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
| Simulation of Effects Of Grain Scale on Al Polycrystal Strength Using Strain Gradient Plasticity Concept |
| ZHOU Li; LI Shouxin; KE Wei |
| Shenyang National Laboratory for Materials Science;Institute of Metal Research; |
引用本文:
周丽; 李守新; 柯伟 . 应变梯度塑性理论模拟晶粒尺寸对铝多晶体强度的影响[J]. 金属学报, 2006, 42(7): 781-784 .
,
,
.
Simulation of Effects Of Grain Scale on Al Polycrystal Strength Using Strain Gradient Plasticity Concept[J]. Acta Metall Sin, 2006, 42(7): 781-784 .
[1] Fleck N A,Muller G M,Ashby M F,Hutchinson J W.Acta Metall Mater, 1994; 42: 475 [2] Stolken J S,Evans A G.Acta Mater,1998; 46: 5109 [3] Lloyd D J. Int Mater Rev, 1994; 39: 1 [4] Xue Z, Huang Y, Li M. Acta Mater, 2002; 50: 149 [5] Fleck N A, Hutchinson J W. J Mech Phys Solids, 1993;41: 1825 [6] Cheong K S, Busso E P, Arsenlis A. Int J Plast, 2005; 21:1797 [7] Huang Y, Xue Z, Gao H, Nix W D, Xia Z C. J Mater Res,2000; 15: 1786 [8] Saha R, Xue Z, Huang Y, Nix W D. J Mech Phys Solids, 2001; 49: 1997 [9] Gao H, Huang Y, Nix W D, Hutchinson J W. J Mech Phys Solids, 1999; 47: 1239 [10] Saada G. Mater Sci Eng, 2005; A400-401: 146; |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|