AZ91D压铸镁合金的三维微观组织模拟
刘志勇;许庆彦;柳百成
清华大学机械工程系; 先进成形制造教育部重点实验室
Three-dimensional Microstructure Simulation of AZ91D Die Casting Magnesium Alloy
引用本文:

刘志勇; 许庆彦; 柳百成 . AZ91D压铸镁合金的三维微观组织模拟[J]. 金属学报, 2006, 42(12): 1291-1297 .

全文: PDF(2123 KB)  
摘要: 针对工程上应用广泛的AZ91D压铸镁合金, 建立了其凝固过程中微观组织演化的数学物理模型. 采用改进的三维微观元胞自动机(CA)模型, 耦合三维溶质场计算,结合压铸镁合金进行了微观组织模拟. 模拟结果再现了在多晶粒同时生长的情况下,初生晶间的溶质扩散、溶质富集直至共晶转变的全部演化过程. 应用此模型模拟了实际AZ91D压铸件不同部位的微观组织, 模拟结果与金相观察结果符合较好.
关键词 : 镁合金,  压铸,  微观组织模拟,  溶质场    
Abstract:Abstract: This paper focuses on the AZ91D die casting magnesium alloy which is used widely in engineering world and proposes a set of mathematical and physical models of microstructure evolution in the solidification process. Coupled with 3D solute concentration field calculation model, a modified 3D micro-scale cellular automaton (CA) model has been founded to simulate the microstructure evolution of AZ91D die casting magnesium alloy. For multi-grains growth simultaneously, this model successfully revealed the whole evolution process of solute diffusion among the primary grains, solute enrichment and the eutectic transformation. The improved model was applied to simulate the microstructure of different parts of the actual AZ91D die casting and simulation results are in good agreement with the experimental.
Key words: Microstructure simulation    Solute concentration field    Magnesium alloy    Die casting
收稿日期: 2006-03-31     
ZTFLH:  TG244  
[1] Zhang P, Zeng D B. J Spec Cast Non-ferrous Alloys, 2000; 6: 55 (张鹏.曾大本.特种铸造及有色合金, 2000;6:55)
[2] Chen Z H. Magnesium Alloy. Beijing: Chemical Industry Press, 2004: 108 (陈振华.镁合金.北京:化学工业出版社, 2004:108)
[3] Liu B C. Chin J Mech Eng, 2000; 11: 67 (柳百成.中国机械工程, 2000;11:67)
[4] Boettinger W J, Coriell S R, Greer A L, Karma A, Kurz W, Rappaz M, Trivedi R. Acta Mater, 2000; 48: 43
[5] Beltran-Sanchez L, Stefanescu D M. Metall Mater Trans, 2003; 34A: 367
[6] Beltran-Sanchez L, Stefanescu D M. Metall Mater Trans, 2004; 35A: 2471
[7] Raghavan S, Krane M J M, Johnson D R. Modeling of Casting, Welding and Advanced Solidification Processes- X, Destin: TMS, 2003: 107
[8] Li Q, Li D Z, Qian B N. Acta Matall Sin, 2004; 40: 1215 (李强,李殿中,钱百年.金属学报, 2004;40:1215)
[9] Zhu M F, Dai T, Li C Y, Hong C P. Sci Chin, 2005; 35E: 673 (朱鸣芳,戴挺,李成允,洪俊杓.中国科学, 2005;35E: 673)
[10] Zhu M F, Hong C P. ISIJ Int, 2002; 42: 520
[11] Wang W, Lee P D, McLean M. Acta Mater, 2003; 51: 2971
[12] ASM Handbook Committee. ASM Handbook, Volume 3: Alloy Phase Diagrams. Metals Park, Ohio: ASM International, 1992: 2.48
[13] Hultgren R, Desai P D, Hawkins D T. Selected Values of the Thermodynamic Properties of Binary Alloys Metals Handbook. Metals Park, Ohio: ASM, 1973: 180
[14] Liu Z, Zhang K, Zeng X Q. Theory and Application of Mg-based Light Alloy. Beijing: China Machine Press, 2002: 47 (刘正,张奎,曾小勤.镁基轻质合金理论基础及其应用.北京:机械工业出版社,2002:47)
[15] Cui Z Q. Metallography and Heat Treatment. Beijing: China Machine Press, 1989: 94 (崔忠圻.金属学与热处理.北京:机械工业出版社,1989:94)
[16] Lu S X, Gu K D, Zheng L S. Non-ferrous Cast Alloy and Melting. Beijing: National Defence Industry Press, 1983: 185 (陆树荪,顾开道,郑来苏.有色铸造合金及熔炼.北京:国防工业出版社, 1983:185)
[17] Zeng R C, Ke W, Xu Y B. Acta Matall Sin, 2001; 37: 673 (曾荣昌,柯伟,徐永波.金属学报, 2001;37:673)
[18] Wang Y S, Zhang Y B, Wang Q D, Ma C J, Ding W J, Zhu Y P. Acta Matall Sin, 2002; 38: 539 (王业双,张咏波,王渠东,马春江,丁文江,朱燕萍.金属学报,2002;38:539)
[19] Xiong S M, Xu Q Y, Kang J W. Modeling and Simulation Technology in Casting Process. Beijing: China Machine Press, 2004: 140 (熊守美,许庆彦,康进武.铸造过程模拟仿真技术.北京:机械工业出版社,2004:140)
[20] Thevoz P H, Desbiolles J L, Rappaz M. Metall Trans, 1989; 20A: 311
[21] Kurz W, Giovanola B, Trivedi R. Acta Metall, 1986; 34: 823
[22] Rappaz M, Thevoz P H. Acta Metall, 1987; 35: 1487
[23] Nastac L. Acta Mater, 1999; 47: 4253
[24] Xu Q Y, Liu B C. Chin J Mech Eng, 2001; 12: 328 (许庆彦,柳百成.中国机械工程,2001;12:328)
[25] Feng W M, Xu Q Y, Liu B C. J Tsinghua Univ, 2003; 43: 605 (冯伟明,许庆彦,柳百成.清华大学学报, 2003;43:605)
[26] Xu Q Y, Feng W M, Liu B C. Acta Metall Sin, 2002; 38: 799 (许庆彦,冯伟明,柳百成.金属学报, 2002;38:799)
[1] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[2] 邵晓宏, 彭珍珍, 靳千千, 马秀良. 镁合金LPSO/SFs结构间{101¯2}孪晶交汇机制的原子尺度研究[J]. 金属学报, 2023, 59(4): 556-566.
[3] 沈朝, 王志鹏, 胡波, 李德江, 曾小勤, 丁文江. 镁合金抗高温氧化机理研究进展[J]. 金属学报, 2023, 59(3): 371-386.
[4] 朱云鹏, 覃嘉宇, 王金辉, 马鸿斌, 金培鹏, 李培杰. 机械球磨结合粉末冶金制备AZ61超细晶镁合金的组织与性能[J]. 金属学报, 2023, 59(2): 257-266.
[5] 唐伟能, 莫宁, 侯娟. 增材制造镁合金技术现状与研究进展[J]. 金属学报, 2023, 59(2): 205-225.
[6] 彭立明, 邓庆琛, 吴玉娟, 付彭怀, 刘子翼, 武千业, 陈凯, 丁文江. 镁合金选区激光熔化增材制造技术研究现状与展望[J]. 金属学报, 2023, 59(1): 31-54.
[7] 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟. 高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能[J]. 金属学报, 2022, 58(5): 660-672.
[8] 孙宝德, 王俊, 康茂东, 汪东红, 董安平, 王飞, 高海燕, 王国祥, 杜大帆. 高温合金超限构件精密铸造技术及发展趋势[J]. 金属学报, 2022, 58(4): 412-427.
[9] 曾小勤, 王杰, 应韬, 丁文江. 镁及其合金导热研究进展[J]. 金属学报, 2022, 58(4): 400-411.
[10] 罗旋, 韩芳, 黄天林, 吴桂林, 黄晓旭. 层状异构Mg-3Gd合金的微观组织和力学性能[J]. 金属学报, 2022, 58(11): 1489-1496.
[11] 李少杰, 金剑锋, 宋宇豪, 王明涛, 唐帅, 宗亚平, 秦高梧. “工艺-组织-性能”模拟研究Mg-Gd-Y合金混晶组织[J]. 金属学报, 2022, 58(1): 114-128.
[12] 刘日平, 马明臻, 张新宇. 块体非晶合金铸造成形的研究新进展[J]. 金属学报, 2021, 57(4): 515-528.
[13] 潘复生, 蒋斌. 镁合金塑性加工技术发展及应用[J]. 金属学报, 2021, 57(11): 1362-1379.
[14] 王慧远, 夏楠, 布如宇, 王珵, 查敏, 杨治政. 低合金化高性能变形镁合金研究现状及展望[J]. 金属学报, 2021, 57(11): 1429-1437.
[15] 王雪梅, 殷正正, 于晓彤, 邹玉红, 曾荣昌. AZ31镁合金表面苯丙氨酸、甲硫氨酸和天冬酰胺诱导Ca-P涂层耐蚀性能比较[J]. 金属学报, 2021, 57(10): 1258-1271.