| TiNi合金不完全相变的温度记忆效应 |
| 郑雁军 崔立山 |
| 石油大学材料科学与工程系; 北京102249 |
|
| Temperature Memory Effect of Partial Transformation in TiNi Alloys |
| ZHENG Yanjun; CUI Lishan |
| Department of Materials Science and Engineering; University of Petroleum; Beijing 102249 |
引用本文:
郑雁军; 崔立山 . TiNi合金不完全相变的温度记忆效应[J]. 金属学报, 2004, 40(9): 915-919 .
,
.
Temperature Memory Effect of Partial Transformation in TiNi Alloys[J]. Acta Metall Sin, 2004, 40(9): 915-919 .
[1] Wei Z G, Sandstrom R. J Mater Sci, 1998; 33: 3743 [2] Wei Z G, Sandstrom R, Miyazaki S. J Mater Sci, 1998;33: 3763 [3] Madangopal K, Banerjee S, Lele S. Acta Metall Mater,1994; 42: 1875 [4] Airoldi G, Riva G. Key Eng Mater, 1990; 48: 5 [5] Airoldi G, Corsi A, Riva R. Mater Sci Eng, 1998; A241:233 [6] Amengual A. Scr Metall Mater, 1992; 26: 1795 [7] Piao M, Otsuka K, Miyazaki S, Horikawa H. Mater TransJIM, 1993; 34: 919 [8] Lin H C, Wu S K, Chou T S, Kao H P. Acta Metall Mater,1991; 39: 2069 [9] Liu Y N, Favier D. Acta Mater, 2000; 48: 3489 [10] Zheng Y J, Cui L S, Zhang F, Yang D Z. J Mater SciTechnol, 2000; 16: 611 [11] Zheng Y J, Cui L S, Zhu D, Yang D Z. Mater Lett, 2000,43(3) : 91 [12] Zheng Y J, Schrooten J, Tsoi K A, Sittner P. Exp Mech,2003; 43: 194 [13] Zheng Y J, Schrooten J, Tsoi K A, Stalmans R. Mater SciEng, 2002; A335: 157 [14] Tong H C, Wayman C M. Acta Metall, 1974; 22: 887 [15] Olson G B, Cohen M. Acta Metall, 1979; 27: 1907 [16] Raghavan V, Cohen M. Acta Metall, 1972; 20: 779 [17] Tadaki T, Kakeshita T, Shimizu K. In: Delaey L, Chan-drasekaran M, eds., Int Conf on Martensitic Transforma-tions(ICOMAT'82) , Heverlee, Belgium: KULeuven, 1982: 191E |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|