| 爆炸喷涂制备NiCrAlY/NiAl/ZrO2-Y2O3体系热障涂层 |
| 武颖娜; 柯培玲; 孙超; 华伟刚; 王福会; 闻立时 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| NiCrAlY/NiAl/ZrO2-Y2O3 Thermal Barrier Coatings Obtained by Detonation Spraying |
| WU Yingna; KE Peiling; SUN Chao; HUA Weigang; WANG Fuhui; WEN Lishi |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
武颖娜; 柯培玲; 孙超; 华伟刚; 王福会; 闻立时 . 爆炸喷涂制备NiCrAlY/NiAl/ZrO2-Y2O3体系热障涂层[J]. 金属学报, 2004, 40(5): 541-545 .
,
,
,
,
,
.
NiCrAlY/NiAl/ZrO2-Y2O3 Thermal Barrier Coatings Obtained by Detonation Spraying[J]. Acta Metall Sin, 2004, 40(5): 541-545 .
[1] Padture N P, Gell M, Jordan E H. Science, 2002; 296:280 [2] Miller R A, Lowell C E. Thin Solid Films, 1982; 95:265 [3] Haynes J A, Ferber M K, Porter W D, Rigney E D. Oxid Met, 1999; 52:31 [4] Rabiei A, Evans A G. Acta Mater, 2000; 48:3963 [5] Ma X Q, Rhyim Y M, Jin H W, Park C G, Kim M C. Corrosion, 1999; 55:805 [6] Wu B C, Chao C H, Chang E. Mater Sci Eng, 1990; A124: 215 [7] Lih W, Chang E, Wu B C, Chao C H. Oxid Met, 1991; 36:221 [8] Wu Y N, Zhang G, Feng Z C, Zhang B C, Liang Y, Liu F J. Surf Coat Technol, 2001; 138:56 [9] Sun J H, Chang E, Wu B C, Tsai C H. Surf Coat Technol, 1993; 58:93 [10] Taylor T A. Surf Coat Technol, 1992; 54/55:53 [11] Kyongjun A, Ravichandran K S, Dutton R E, Semiatin S L. J Am Ceram Soc, 1998; 82:399 [12] Hasselman D P H. J Compos Mater, 1978; 12:403 [13] McPherson R. Thin Solid Film, 1984; 112:89 [14] Wu Y N, Hua W G, Ji A L, Wang F H, Sun C, Wen L S. Acta Metall Sin, 2002; 38:1082(武颖娜,华伟刚,纪爱玲,王福会,孙超,闻立时.金属学报,2002;38:1082) [15] Wu Y N, Wang F H, Hua W G, Gong J, Sun C, Wen L S. Surf Coat Technol, 2003; 166:189 [16] Busso E P, Lin J, Sakurai S, Nakayama M. Acta Mater, 2001; 49:1515 [17] Zhu R Z, He Y D, Qi H B. High Temperature Corrosion and Materials of High Temperature Corrosion Resistance. Shanghai: Shanghai Scientific and Technical Publishers, 1995:340(朱日彰,何业东,齐慧滨.高温腐蚀及耐高温腐蚀材料.上海:上海科学技术出版社,1995:340) [18] Bobeth M, Pompe W, Shumann E, Ruhle M. Acta Metall Mater, 1992; 40:2669 |
|