软接触结晶器电磁连铸保护渣道的动态压力 |
雷作胜; 任忠鸣; 阎勇刚; 邓康 |
上海大学上海市钢铁冶金新技术应用开发重点实验室; 上海 200072 |
|
Mold Flux Channel Dynamic Pressure in Electromagnetic Continuous Casting |
LEI Zuosheng; REN Zhongming; YAN Yonggang; DENG Kang |
Shanghai Enhanced Laboratory of Ferro-Metallurgy; Shanghai University; Shanghai 200072 |
引用本文:
雷作胜; 任忠鸣; 阎勇刚; 邓康 . 软接触结晶器电磁连铸保护渣道的动态压力[J]. 金属学报, 2004, 40(5): 546-550 .
,
,
,
.
Mold Flux Channel Dynamic Pressure in Electromagnetic Continuous Casting[J]. Acta Metall Sin, 2004, 40(5): 546-550 .
[1] Asai S. Tetsu Hagané, 1989: 75:32(浅井 滋生.铁钢,1989:75:32) [2] Li T J, Sassa K, Asai S. ISIJ Int, 1996; 36:410 [3] Ren Z M, Dong H F, Dent K, Jiang G C. ISIJ Int, 2001; 41:981 [4] Na X Z, Zhang X Z, Qiu S T, Can Y. Acta Metall Sin, 2002; 38:105(那贤昭,张兴中,仇圣桃,干勇.金属学报,2002;38:105) [5] Toh T, Takeuchi E, Hojo M, Kawai H, Matsumura S. ISIJ Int, 1997; 37:1112 [6] Ayata K, Miyazawa K, Takeuchi E, Bessho N, Mori H, Tozawa H. In: Asai S, ed., The 3rd Int Syrup on Electromagnetic Processing of Material, Nagoya: Iron Steel Inst Japan, 2000:376 [7] Takeuchi E, Brimacombe J K. Metall Trans, 1984; 15B: 493 [8] Nakata H, Etay J. ISIJ Int, 1992; 32:521 [9] Miyoshino I, Takeuchi E, Yano H, Sakane J, Saeki T, Kajioka H. ISIJ Int, 1989; 29:104 [10] Bikerman J J. Physical Surface. New York: Academic Press, 1970:12 [11] American Society for Metals. Metals Handbook. Vol. 2, 9th ed., Metals Park, Ohio: ASM International, 1990: 1093 [12] Zhang X Y, Qi B M, Zhu X L. Applied Chemic Handbook. Beijing: National Defence Industry Press, 1986:322(张向宇,戚保民,朱鑫林.实用化学手册.北京:国防工业出版社,1986:322) [13] Sumi I, Sassa K, Asai S. Tetsu Hagané, 1992; 78:447(鹫见 郁宏,佐佐 健介,浅井 滋生.铁钢,1992;78:447) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|