| M963铸造镍基高温合金的液态结构分析 |
| 殷凤仕 孙晓峰 |
| 中国科学院金属研究所 110016 |
|
引用本文:
殷凤仕; 孙晓峰 . M963铸造镍基高温合金的液态结构分析[J]. 金属学报, 2003, 39(5): 530-532 .
[1] Zhang L, Bian X F, Ma J J. Foundry, 1995; (10) : 7(张林,边秀房,马家骥.铸造,1995;(10) :7) [2] Cheng G, Cai Y W, Li J G, Fu H Z. J Hebei Univ Sci Technol, 1998; 19: 6(陈光,蔡英文,李建国,傅恒志.河北科技大学学报,1998;19:6) [3] Gui Z L. Aviat Product Eng, 1995; (4) : 12(桂忠楼.航空制造工程,1995;4:12) [4] Chen G, Yu J W, Xie F Q, Fu H Z. Acta Metall Sin, 2001; 37: 488(陈光,俞建威,谢发勤,傅恒志.金属学报,2001;37:488) [5] Yin F S Sun X F, Li Y B, Yu Y, Zheng Q, Guan H R, Hu Z Q. Acta Metall Sin, 2003; 39: 75(殷凤仕,孙晓峰,李耀彪,于洋,郑启,管恒荣,胡壮麒.金属学报,2003;39:75) [6] Pan X M, Bian X F, Qin J Y, Wang W M. Acta Phys-Chim Sin, 2001; 17: 708(潘学民,边秀房,秦敬玉,王伟民.物理化学学报,2001;17:708) [7] Bian X F, Qin J Y, Wang W M, Liu X F, Ma J J. Acta Metall Sin, 1999; 35: 19(边秀房,秦敬玉,王伟民,刘相法,马家骥.金属学报,1999;35:19) [8] Cong H R, Bian X F, Li H, Wang L. Acta Phys-Chim Sin, 2002; 18: 39(从红日,边秀房,李辉,王丽.物理化学学报,2002;18:39) [9] Cong H R, Bian X F, Li H. Acta Chim Sin, 2002; 60: 287(从红日,边秀房,李辉.化学学报,2002;60:287) [10] Burton C J, Boesch W J. Met Prog, 1975; 108: 121 [11] Liu L, Zhen B L, Banerji A, Reif W, Sommer F. Scr Metall Mater, 1994; 30: 593 [12] Hoyer W, Jodicke R. J Non-Cryst Solids, 1995; 193: 102 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|