Mg-Y-Nd合金的蠕变行为及其微观机制 |
沙桂英; 韩恩厚; 于涛; 徐永波; 刘路; 高国忠 |
中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
引用本文:
沙桂英; 韩恩厚; 于涛; 徐永波; 刘路; 高国忠 . Mg-Y-Nd合金的蠕变行为及其微观机制[J]. 金属学报, 2003, 39(10): 1025-1030 .
[1] Mohri T, Mabuchi M, Saito N, Nakamura M. Mater Sci Eng, 1998; A257: 287 [2] Bae D H, Kim D H. Magnesium Technology, In: KaplanH I ed, TMS, The Minerals, Metals and Materials Society,2002: 141 [3] Wang Q D, Lu Y Z, Zeng X Q, Ding W J, Zhu Y P. SpecialCasting and Nonferrous Alloy, 1999; 1: 40(王渠东,吕宜振,曾小勤,丁文江,朱燕萍.特种铸造及有色合金,1999;1:40) [4] Moreno I P, Nandy T K, Jones J W, Allison J E, Pollock T M. Magnesium Technology, In : Kaplan H I ed, TMS, The Minerals, Metals and Materials Society, 2002: 111 [5] Abe E, Takakura H, Singh A, Tsai A P. J Alloys and Compds, 1999; 283: 169 [6] Maruyama K, Suzuki M, Sato H. Metall Mater Trans,2002; 33A: 875 [7] Guo X T, Li P J, Zeng D B. Transactions of Materialsand Heat Treatment, 2001; 22(Suppl): 115(郭旭涛,李培杰,曾大本.材料热处理学报,2001;22(Suppl):115) [8] Nie J F, Muddle B C. Acta Mater, 2000; 48: 1691 [9] Khosroshahi R A. Magnesium Alloys and Their Applications, In: Kainer K U ed, WILEY-VCH, New York, 2000:711 [10] Suzuki M, Sato H, Maruyama K, Oikawa H. Mater SciEng, 1998; 252A: 248 [11] Nie J F, Muddle B C. Scr Mater, 1999; 40: 1089 [12] Apps P J, Karimzadeh H, King J F, Lorimer G W. Scr Mater, 2003; 48: 1023 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|