| 激光金属成形定向凝固显微组织及成分偏析研究 |
| 冯莉萍 黄卫东 李延民 杨海欧 林鑫 |
| 西北工业大学凝固技术国家重点实验室;西安710072 |
|
引用本文:
冯莉萍; 黄卫东; 李延民; 杨海欧; 林鑫 . 激光金属成形定向凝固显微组织及成分偏析研究[J]. 金属学报, 2002, 38(5): 501-506 .
[1]Pan Q Y. J Mater Sci Lett, 1996; 15: 2112 [2]Cline H E. Metall Trans, 1984; 14A: 1013 [3]Cline H E. Mater Sci Eng, 1984: 65 [4]Abbott D H, Arcella F G. Adv Mater Proc, 1998: 29 [5] Schlienger E, Dimos D, Griffith M, Michael J, Oliver M, Romero T, Smugeresky J. Proceedings of the Third Pacific Rim International Conference on Advanced Materials and Processing (Vol.I), Hawaii. USA: 1998: 1581 [6] Keicher D M, Smugeresky J E, Romero J A, Griffith M L, Harwell L D. SPIE, 2293: 91 [7] Gaumann M, Bezencon C, Canalis P, Kurz W. Acta Mater, 2001; 49: 1051 [8] Barth M, Wei B, Herlach D M, Feuerbacher B. Mater Sci Eng, 1994; A178: 305 [9]Kurz W, Fisher D J. Fundamentals of Solidification(4th eds). Switzerland: Trans Tech Publication, 1984: 70 [10]Li Y M. PhD Thesis, Northwestern Polytechnical Univer-sity, Xi'an, 2001 (李延民. 西北工业大学博士学位论文.西安.2001) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|