| 表面效应对纳米铜杆拉伸性能影响的原子模拟 |
| 梁海弋 倪向贵 王秀喜 |
| 中国科学技术大学力学与机械工程系;合肥230026 |
|
引用本文:
梁海弋; 倪向贵; 王秀喜 . 表面效应对纳米铜杆拉伸性能影响的原子模拟[J]. 金属学报, 2001, 37(8): 833-836 .
[1] Basant Zdenek. Er-Ping Chen. Adv Mech, 1999; 29: 383 [2] Brenner S S. J Appl Phys, 1956; 27: 1484 [3] Schiotz, Francesco D.Di. Karsten W. Jacobsen. Nature,1998, 391: 561 [4] Craihead H G. Scienee. 2000. 290: 1532 [5] Hafner J. Acta Miter, 2000; 48: 71 [6] Allen M P. Tildesley D J. Computer Simulation of Liq-uids. Oxford: Clarendon Press, 1987: 284 [7] Masao Doyama, Kogure Y. Comput Mater Sci, 1999; 14.80 [8] Parrinello M, Rahman A. J Appl Phys, 1981; 52: 7182 [9] Cammarata R C. Prog Surf Sci, 1994; 46(1): 1D |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|