Nd60Fe30Al10大块非晶的制备及其热稳定性
邱克强  王爱民  张庆生  张海峰  丁炳哲  胡壮麒
中国科学院金属研究所快速凝固非平衡合金国家重点实验室;沈阳110016
引用本文:

邱克强; 王爱民; 张庆生; 张海峰; 丁炳哲; 胡壮麒 . Nd60Fe30Al10大块非晶的制备及其热稳定性[J]. 金属学报, 2001, 37(8): 829-832 .

全文: PDF(173 KB)  
摘要: 采用熔渣包覆水淬法获得了直径为6 mm,长度为50 mm的非晶Nd60Ee30Al10合金,并对其非晶形成能力进行了研究.在三元系非晶合金中,除Pd基合金外,这是目前所报道的采用水淬法所能获得的最大尺寸的非晶合金.对Nd70Fe20Al10,在同样的条件下可获得直径为3 mm,长度为50 mm的部分非晶组织.与普通铜模铸造方法所获得的临界直径相比,前者提高了2 mm,而后者降低了4 mm.利用DTA和DSC对Nd60Fe30Al10合金的熔点和形成能力进行了分析,所计算的临界冷却速率为0.55 K/s,表明该合金具有较大的非晶形成能力.表观晶化能计算结果和DSC曲线分析表明,Nd60Fe30Al10非晶的热稳定性较低.
关键词 : Nd60Fe30Al10大块非晶合金,  熔渣包覆水淬法    
Key words:
收稿日期: 2000-12-22     
ZTFLH:  TF649  
[1] Inoue A, Kita K, Zhang T, Masumoto T. Mater TransJIM,1989; 30: 722
[2] Inoue A, Zhang T, Nishiyama N, Ohba K, Masumoto T.Mater Trans JIM 1993; 34: 1234
[3] Inoue A, Zhang T, Masumoto T. Mater Trans JIM 1990;31: 425
[4] Inoue A, Kato A, Zhang T, Kim S G, Masumoto T. MaterTrans JIM 1991; 32: 609
[5] Inoue A, Nakmaura T, Nishiyama N, Masumoto T. MaterTrans JIM 1992; 33: 937
[6] Inoue A. Nakmaura T, Sugita T, Zhang T, Masumoto T.Mater Trans JIM, 1993; 34: 351
[7] Inoue A, Zhang T. Metals, 1994; 64: 3-47
[8] Inoue A, Yokoyama Y, Shinohara Y, Masumoto T. MaterTrans JIM, 1994; 35: 923
[9] Yokoyama Y, Inoue A. Mater Trans JIM, 1995; 36: 1398
[10] Inoue A, Zhang T. Mater Trans JIM 1995; 36: 1184
[11] Inoue A, Zhang T. Mater Trans JIM 1996; 37: 185
[12] Inoue A, Zhang T. Takeuchi A, Zhang W. Mater TransJIM 1996; 37: 636
[13] Lin X H, Johnson W L, Khim W K. Mater Trans JIM,1997; 38: 473
[14] Inoue A, Nishiyama N and Kimura H. Mater Trans JIM,1997; 38: 179
[15] Lu Z P, Li Y, Ng S C. J Non-Cryst Solids, 2000; 270: 103
[16] Inoue A, Zhang T, Zhang W, Takeuchi A. Mater TransJIM 1996; 37: 99
[17] Lu Z P, Tan H, Li Y, Ng S C. Scr Mater,2000; 42: 667
[18] He Y, Schwarz R B, Archuleta J I. Appl Phys Lett, 1996;69: 1861
[19] Turnbull D. Contemp Phys, 1969; 10: 473
[20] Chen L C, Spaepen F. Nature, 1988; 336: 366
[21] Lu Z P, Li Y, Ng S C, Feng Y P. In: Johnson W L, InoueA, Liu C T eds., Bulk Metallic Glasses, Material ResearchSociety 1999: 205
[22] Kissinger H. Anal Chem, 1957; 29: 1702
[23] Qu X D, Sun W S, Zhang F J, Yang Y K, Xu D L, QuanM X. Met Funct Mater, 1998; 5: 215(曲向东,孙文声,张凤军,杨耀库,徐敦良,全明秀,金属功能材料,1998;5:215)
[24] Greer A L. Nature, 1993; 366: 25
[25] Inoue A, Zhang T. Mater Sci Eng, 1997; 226-228A: 393
[26] Fan G J, Loser W, Roth S, Eckert J, Schultz L. J MaterRes, 2000; 15: 1556B
No related articles found!