α-Al2O3,TiB2颗粒增强铝基复合材料的XD合成 |
朱和国 王恒志 吴申庆 |
东南大学材料科学与工程系;南京210006 |
|
引用本文:
朱和国; 王恒志; 吴申庆 . α-Al2O3,TiB2颗粒增强铝基复合材料的XD合成[J]. 金属学报, 2001, 37(3): 321-324 .
[1] Zhu H G, Wu S Q. Mater Rev, 1998; 12: 61 (朱和国,吴申庆.材料导报,1998;12: 61) [2] Wu S Q, Zhu H G, Tjong S C. Metall Trans, 1999; 30A:243 [3] Wood J V, Davies P, Kellie J L F. Mater Sci Techn, 1993;9: 833 [4] Dubey S, Lederich R J, Boyejo W O S. Metall MaterTrans, 1997; 28A: 2037 [5] Zhang E L, Zeng S Y, Yang B, Li Q C, Ma M Z. MetallTrans, 1999; 30A: 1147 [6] Tong X C. J Mater Sci, 1998; 33: 5363 [7] Lu W J, Zhang X N, Zhang D, Wu R J, Bian Y J, FangP W. Acta Metall Sin,1999;35:536 (吕维洁,张小农,张获,吴人洁,卞玉君,方平伟.金属学报.1999;35:536) [8] Biswas S, Varin R A. Metall Mater Trans, 1996; 27: 71 [9] Zhao Z M, Ye M H, Du X K, Wang J J, Zhang R. Foundry.2000: 4: 189 (赵忠民,叶惠民,杜绝心康,王建江,张龙.铸造.2000;4:189) [10] Ma Z Y, Lu Y X, Bi J. Acta Metall Sin, 1999; 1: 93 (马宗义,吕毓雄,毕敬.金属学报.1999;1:93) [11] Ma Z Y, Li J H, Li S X, Ning X G, Lu Y X, Bi J. J MaterSci, 1996; 31: 741 [12] Ye D R. Hand Book of Thermodynamical Data for Inorganic Substance. Beijing: Metallurgy Industry Press,1981: 25 (叶大伦.实用无机物热力学数据手册.北京:冶金工业出版社,1981:25) [13] Munir Z A. Ceram Bull, 1988; 67: 342 [14] Purch S, Michael J Koczak. Mater Sci Eng, 1991; 144A:37 [15] Nakata H J. Mater Sci, 1995; 30: 1719 [16] Chen Z Y, Chen Y Y, Shu Q, An G Y, Yang R, Liu Y Y,Li D. Chin J Mater Res, 2000; 14, Supple: 68 (陈子勇,陈玉勇,舒群,安阁英,杨锐,刘羽寅,李东.材料研究学报,2000;14 Supple:68) [17] Yang B, Wang Y Q, Zhou B L. Metall Mater Trans. 19981;29B: 635 [18] Atoda T, Higashi I, Kobayashi M. Sci Paper InstitutionPhysiology Chem Res, 1967; 61: 92 [19] Zhang S Y, Chen Y Y, Shen G J, Cao F X, Li Q C. TheChin J Nonferrous Met, 1999; 9 supple 1: 131 (张淑英,陈玉勇,沈光骏,曹福祥,李庆春.中国有色金属学报, 1999; 9 supple 1: 131) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|