| Ti合金电子束焊接三维温度场计算 |
| 刘敏 康继东 李瑜 陈士煊 |
| 山东大学材料学院;济南250061 |
|
引用本文:
刘敏; 康继东; 李瑜; 陈士煊 . Ti合金电子束焊接三维温度场计算[J]. 金属学报, 2001, 37(3): 301-306 .
[1] Admas C M. Welding J, 1958; 37: 210 [2] Christensen N, Davies V L, Gjermunclsen K. Welding J,1965; 12: 54 [3] Swift-Hook D T, Gick A E F. Welding J, 1 973; 52: 492 [4] Wei P S, Shian M D. ASME J Heat Trasfer, 1993; 115:848 [5] Wei P S, Ho C Y, Shian M D, Hu C L. Int J Heat Mass,1997; 40: 2283 [6] Aeronautics Material Research Institute of Beijing, Material Datum Handbook for Aeroengine Design, Shenyang:Aeroengine Research Institute Press, 1990: 1206 (北京航空材料研究所,航空发动机设计用材料数据手册,沈阳:航空发动机研究所出版,1990:1206)( |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |