| 2Cr13钢激光熔凝处理的过渡区组织分析 |
| 邵天敏 蔺秀川 袁伟东 |
| 清华大学摩擦学国家重点实验室;北京100084 |
|
引用本文:
邵天敏; 蔺秀川; 袁伟东 . 2Cr13钢激光熔凝处理的过渡区组织分析[J]. 金属学报, 2001, 37(10): 1040-1044 .
[1] Escudero M L, Bello J M. Mater Sci Eny, 1992; 11A: 227 [2] Colaco R, Vilar R. Surf Eng, 1996; 12: 319 [3] Yang D H. Tribiology, 1994; l4(1): 12(杨德华.摩擦学学报.1994;14(1):12) [4] Bai X D, Xu J, Fan Y D. J Tsinghua Univ (Sci Technol),1998; 38(12): 35(白新德,徐 健,范玉殿.清华大学学报(自然科学版),1998;38(12):35) [5] Liu J L. Heat Treatment by High-Energy Beam. Beijing:China Machine Press, 1997: 212(刘江龙·高能束热处理.北京:机械工业出版社,1997:277) [6] Guan Z Z. Handbook of Laser Material Processing. Bei-(关振中.激光加工工艺手册.北京:中国计量出版社,1998:153) [7] Luo G X. Trans Met Heat Treat, 1999; 20(3): 48(罗耕星.金属热处理学报,1999;20(3):48) [8] Cui K. Steel and Non-Ferrous Metal. Beijing: Metallur-gical Industry Press, 1980: 258 (崔 ■. 钢铁材料及有色金属材料.北京:冶金工业出版社, 1980:258) [9]Beres L WeldJ, 1998;77:273s |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|