| 毛萍莉 杨柯 苏国跃 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
毛萍莉; 杨柯; 苏国跃 . 铸态奥氏体不锈钢的热变形行为[J]. 金属学报, 2001, 37(1): 39-41 .
[1] Kato K, Saito Y, Sakai T. Trans ISIJ, 1984; 24: 1050 [2] Ryan N D, McQueen H J, Jonas J J. Can Metall Q, 1983;22: 369 [3] Maki T, Akasaka K, Okuno K. Trans ISIJ, 1982; 22: 253 [4] Ouchi C, Okita T. Trans ISIJ, 1982; 22: 543 [5] Ryan N.D, McQueen H J. Can Metall Q, 1990; 29: 147 [6] Ryan N D, McQueen H J. Mate Proces Technol, 1990; 121:177 [7] Hu D L. Metal Science. Xi'an: Northwestern Polytechnical University Press, 1982: 282(胡德林.金属学.西安:西北工业大学出版社,1982:282) [8] Roberts W. Deformation,Processing and Structure. Metals Park, Ohio: ASM, 1984: 109 [9] Sun B R, Zeng X Z. Acta Metall Sin, 1988; 24: B109| |
|