| 单晶Ni基合金高温蠕变期间γ’相定向粗化驱动力的有限元分析 |
| 田素贵 陈昌荣 |
| 沈阳工业大学材料科学与工程学院; 沈阳 110023 |
|
引用本文:
田素贵; 陈昌荣 . 单晶Ni基合金高温蠕变期间γ’相定向粗化驱动力的有限元分析[J]. 金属学报, 2000, 36(5): 465-471 .
[1] Tien J K, Copley S M. Metall Trans,1971; 2: 215 [2] Socrate S, Parks D M. Acta Metall Mater, 1993; 41: 2185 [3] Pollock T M, Argon A S. Acta Metall Mater 1994; 42(6):1859 [4] Nabarro F R N, Cress C M, Kotschy P. Acta Metall Mater,1996; 44: 3189 [5] Glatzel U, Feller-Kniepmeier M. Scr Mater,1989; 23:1839 [6] Pollock T M, Argon A S. Acta Metall Mater, 1994; 40: 1 [7] Muller L, Glatzel U, Feller-Kniepmeier M. Acta MetallMate,1992; 40: 1321 [8] Tian S G, Zhou H H, Zhang J H, Yang H C, Xu Y B, HuZ Q. Acta Metall Sin, 1998; 34 (6): 591(田素贵,周惠华,张静华,杨洪才,徐永波,胡壮麒.金属学报,1998;34(6:591) [9] Tian S G, Zhou H H, Zhang J H, Yang H C, Xu Y B, HuZ Q. Acta Metall Sin, 1998; 34(12): 1261(田素贵,周惠华,张静华,杨洪才,徐永波,胡壮麒.金属学报,1998;34(12):1261) [10] Ohashi T, Hidaka K, Imano S. Acta Mater,1997; 45(5):1801 [11] Eshelby J D. Proc R Soc, 1952; A241: 376 [12] Eshelby J D. Prog Solid Mech, 1961; 2: 87 [13] Buffiere J Y, Cheynet M C, Ignat C. Scr Mater, 1996;34(3): 349 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|