|
|
|
| 板状晶粒不稳定外形的有限元分析 |
| 黄佩珍 李中华 |
| 西安交通大学建筑工程与力学学院; 西安 710049 |
|
引用本文:
黄佩珍; 李中华 . 板状晶粒不稳定外形的有限元分析[J]. 金属学报, 2000, 36(5): 459-464 .
[1] Robertson W M. J Appl Phys, 1971; 42: 463 [2] Binh V T, Moulin Y, Uzan R, Dreschler M. Sauf Sci,1976;57: 184 [3] Lee J K, Courtney T H. Metall Trans, 1989; A20: 1385 [4] Cocks A C F, Gill S P A. Acta Matet 1996; 44(12): 4765 [5] Needleman A, Rice J R. Acta Metall, 1980; 28: 1315 [6] Suo Z, Wang W. J Appl Phys, 1994; 76: 3410 [7] Sun B, Suo Z. Acta Mater 1997; 45(12): 4953 [8] Malzahn Kampe J C, Courtney T H, Leng Y. Acta Metall,1989; 37(7): 1735 [9] Miller K T, Lange F F. Acta Metall, 1989; 37: 1343 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|