| WC硬质合金堆焊材料界面组织结构和力学性能 |
| 邹增大 王新洪 |
| 山东工业大学材料学院;济南 250061 |
|
引用本文:
邹增大; 王新洪 . WC硬质合金堆焊材料界面组织结构和力学性能[J]. 金属学报, 2000, 36(12): 1279-1283 .
[1] Zou X M. Rear Met Cem Carbide, 1995; 3: 11(邹序枚.稀有金属与硬质合金,1995;3:11) [2] Wang X H, Li Y J, Zou Z D, Liu X M. Weld Technol,1999: (6): 25(王新洪,李亚江,邹增大,刘雪梅.焊接技术,1999;(6):25) [3] Charles Mayer A. Weld Design Fabr, 1982; 55: 61 [4] Zhang S S, Wang Z P, Dong X Q. J Shenyang PolytechUniv, 1991; 13: 43(张树生,王志平,董晓强.沈阳工业大学学报,1991;13:43) [5] Gao F, Zhao Y L, Yang R L, Li L J. J Chin Coal Soc,1996; 21: 85(高峰,赵艳玲,杨瑞林,李力军.煤炭学报,1996; 21:85) [6] Hao H Q Wang Y L, Jin Z H, Wang X T. J Xi'an JiaotongUniv, 1994; 28(7): 67(浩宏奇,王永兰,金志浩,王笑天.西安交通大学学报,1994;28(7):67) [7] McDonald G. Thin Solid Films, 1980; 73: 491 [8] Konyashin I Y. Mater Sci Eng, 1997; 230A: 213 [9] Zou X M. Cem Carbide, 1995; 12: 183 |
|