| 原位电阻法研究高温器件焊面多层金属膜间的扩散 |
| 杜黎光 肖克来提 |
| 上海新代车辆技术有限公司;上海 200050 |
|
引用本文:
杜黎光; 肖克来提 . 原位电阻法研究高温器件焊面多层金属膜间的扩散[J]. 金属学报, 2000, 36(12): 1275-1278 .
[1] Freytage J, Wennemuth I. In: Zhang M, Tu K N eds., Proc 5th Int Conf on Solid-State and Intergrated CircuitTechnology, Beijing: Electronics Industry Press, 1998: 219 [2] Fisher J S, Hall P M. Proc IEEE, 1971; 59: 1418 [3] Morabito J M, Thomas J H, Lesh N G. IEEE Trans PartsHybrids Packag, 1975; 11: 253 [4] Tisone T C, Drobek J. J Vac Sci Technol, 1971; 9: 271 [5] Poate J M, Turner P A, DeBonte W J. J Appl Phys, 1975;46: 4275 [6] Feldman I C, Mayer J W. Fundamentals Of Surface andThin Film Analysis. New York: Elsevier Science Publishing Co Inc, 1986: 163 [7] Vanhecke B, Roggen J, Beyne E, Deceuninck W, Deschepper L, Stals L. VTE, 1992; 4: 64 [8] Hall P M, Morabito J M, Poate J M. Thin Solid Film,1976; 33: 107F |
|