| LY12铝合金的再结晶织构、晶界特征分布及抗腐蚀性能 |
| 王轶农 武保林 |
| 东北大学材料与冶金学院; 沈阳 110006 |
|
引用本文:
王轶农; 武保林 . LY12铝合金的再结晶织构、晶界特征分布及抗腐蚀性能[J]. 金属学报, 2000, 36(10): 1085-1088 .
[1] Watanabe T. Res tech, 1984; 11: 47 [2] Zuo L, Watanabe T, Esling C. Z Metallkd, 1994; 85: 554 [3] Aust K T, Erb U, Palumbo G. Mater Sci Eng, 1994; A178:329 [4] Watanabe T. Moter Sci Forum, 1993; 126: 295 [5] Liang Z D, Xu J Z, Wang F. Three-Dimensional Orientation Analvsis of Textured Materials - ODF Analysis. Shenyang: Northeast University of Technology Press,1986: 108(梁志德,徐家桢.王福.织构材料的三线取向分析术──ODF分析.沈阳:东北工学院出版社,1986:108) [6]Vatne H E, Daaland O, Nes E. Mater Sci Forum, 1994;157-162: 1087 [7] Duggan B J. Acta Metall Mater 1993; 41: 1921 [8] Wang Y N. PhD Thesis, Northeastern University,Shenyang, 2000(王轶农.东北大学博士学位论文,沈阳.2000) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |