Al67Mn8Ti24Nb1金属间化合物亚稳态粉末热压成形后的组织结构及性能 |
傅云义 胡赓祥 孙祖庆 |
上海交通大学材料科学系; 上海 200030 |
|
引用本文:
傅云义; 胡赓祥; 孙祖庆 . Al67Mn8Ti24Nb1金属间化合物亚稳态粉末热压成形后的组织结构及性能[J]. 金属学报, 1999, 35(8): 856-860 .
[1] Yamaguchi M, Umakoshi Y, Yamane T. Philos Mag, l987;A55: 301 [2] Morris D G, Lerf R. Philos Mag, 1991; A63: 1195 [3] Nic J P, Mikkola D E. In: Johnson L A, Pope D P, Stiegler J D eds, High-Temperature Ordered Intemetallic Alloys IV.Pittsburgh, PA: Materials Research Society, 1991. 697 [4] Anton D L, Duhn D N, Giamei A F. J Miner Met Mater Soc, 1989; 41: 12 [5] Chen X F, Chen S P, Wu X H, Fang L H, Hu G X. Mater Sci Eng, 1992; A153: 370 [6] Lnui H, Luzzi D E, Poter W D, Pope D P, Vitek V, Yam-aguchi M. Philos Mag, 1992; A65: 245 [7] Kumar K S, Brown S A. Acta Metall Mater, 1992; 26: 1923 [8] Kumar K S, Brown S A. Philos Mag. 1992, A65. 91 [9] Hu G X, Chen S P, Wu X H, Chen X F. J Mater Res, 1991.6: 957 [10] Fu Y Y, Hu G X, Yang W Y, Sun Z Q. Acta Metall Sin.1999; 35: 600 博云义,胡赓样、杨王 ,孙祖庆,金属学报19992 35:600) [11] Brown S A, Kumar K S. Whittenberger J D. Scr Metall Mater, 1996; 24: 2001 [12] Zhang S, Nic J P, Mikkola D E. Scr Metall Mater, 1990. 24.1441 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|