| 二元复合稀土钨电极材料的性能 |
| 聂祚仁 周美玲 陈颖 张久兴 左铁镛 |
| 北京工业大学材料科学与工程学院; 北京 100022 |
|
引用本文:
聂祚仁; 周美玲; 陈颖; 张久兴; 左铁镛 . 二元复合稀土钨电极材料的性能[J]. 金属学报, 1999, 35(3): 334-336 .
[1] Matsuda F, Ushio M, Sadek A A. Trans Jpn Weld Soc, 1990,21: 3 [2] Nie Z R, Zhou M L, Zhang J X, Chen Y, Zuo T Y. Rare MetMater Eng, 1990, 21: 3)(聂祚仁,周美玲,张久兴,陈颖,左铁镛.稀有金属材料与工程,1997,26:1) [3] Nie Z R, Zhou M L, Zhang J X, Chen Y, Shi D Y, Zuo T Y.J Beijing Polytechnic Unly, 1998, 24(2): 28(聂祚仁,周美玲,张久兴,陈颖,施定远,左铁镛.北京工业大学学报,1998,24(2):28) [4] Jian H Z. Electric Are and Electroslag Weld. Beijing: Mechanical Industry Press, 1982: 10(姜焕中.电弧焊与电渣焊.北京:机械工业出版社,1982:10) |
|