| 压痕诱发单晶Si非晶化相变区的三维空间分布结构 |
| 吴亚桥 徐永波 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室;沈阳 110015 |
|
引用本文:
吴亚桥; 徐永波 . 压痕诱发单晶Si非晶化相变区的三维空间分布结构[J]. 金属学报, 1999, 35(3): 289-291 .
[1] Clarke D R, Kroll M C, Kirchner P D, Cook R F, Hockey BJ. Phys Rev Lett, 1988; 60: 2156 [2] Page T F, Oliver W C, McHargue C J. J Mater Res, 1992;7: 450 [3] Callahan D L, Morris J C. Js Mater Res, 1992; 7: 1614 [4] Susuki T, Ohmura T. Philos Mag, 1996; A74: 1073 [5] Johansson S, Schweitz J A. J Am Ceram Soc, 1988; 71: 617 [6] Saka H, Abe S. J Electron Microsc, 1997; 46: 45 [7] Giannakopoulos A E, Larsson P L, Vestergaard R. Int JSolids Struct, 1994; 31: 2679~ |
|