| 定向凝固镍基高温合金的高温蠕变 |
| 袁超;郭建亭;杨洪才;王淑荷 |
| 中国科学院金属研究所;沈阳;110015;东北大学材料与冶金学院;沈阳;110006;中国科学院金属研究所;沈阳;110015;东北大学材料与冶金学院;沈阳;110006;中国科学院金属研究所;沈阳;110015 |
|
| HIGH TEMPERATURE CREEP OF A DIRECTIONALLY SOLIDIFIED Ni-BASE SUPERALLOY |
| YUAN Chao; GUO Jianting; YANG Hongcai; WANG Shuhe( Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015 School of Materials Science and Metallurgy; Northeastern University; Shenyang 110006)Correspondent. Guo Jianting; professor Tel: 25843531-55493; Fax: (024)23891320;E-mail: jtguo .imr.ac.cn |
引用本文:
袁超;郭建亭;杨洪才;王淑荷. 定向凝固镍基高温合金的高温蠕变[J]. 金属学报, 1998, 34(8): 858-863.
,
,
,
.
HIGH TEMPERATURE CREEP OF A DIRECTIONALLY SOLIDIFIED Ni-BASE SUPERALLOY[J]. Acta Metall Sin, 1998, 34(8): 858-863.
1 Sims C T, Stoloff N S, Hagel W C. Superulloys II New York: John Wiley and Sous Inc, 1987: 123 2 Mackay R A, Maiey R D. Metall Trans, 1982; 13A: 1747 3 Nathal M V, Ebert L J. Metall Trans, 1985; 16A: 427 4 Pollock T M, Argon A S. Acta Metall Mater 1992; 40: 1 5 Rouault-Rogez H, Dupeux M, Ignat M. Acta Metall Mater 1994; 42: 3137 6 Dennison J P, Holmes P D, Wilshire B. Mater Sci Eng, 1978; 33: 35 7 Versnyder F L, Shank M E. Mater Sci Eny, 1970; 6: 213 8 Yuan C, Guo J T, Yang H C, Wang S H. J Mater Sci Tech, 1998; 14(3): 219 9 Mishra R S, Singh S P, Sriramawurthy A M, Pandey M C. Mater Sci Tech, 1995; 11: 341 10 Scarlin R B. Metall Trans, 1976; 7A: 1535 11 Mukherjee A K, Bird J E, Dorn J E. Trans ASM 1969; 62: 155 12 Guo Jianting, Ranucci D, Picco E, Strocchi P M. Metall Trans, 1983; 14A: 2329 13 Tien J K, Coply S M. Metall Trans, 1971; 2A: 215 14 Svetlov I L, Golvovko B A, Epishin A I, Abalakin N P. Scri Metall Maten 1992; 26: 1353 15 袁超,郭建亭,杨洪才,王淑荷,金属学报, 1998; 34(7): 689(Yuan C, Guo J T, Yang H C, Wang S H. Acta Metall Sin, 1998; 34(7): 689) 16 Monkman F C, Grant J. Proc ASTM 1956; 56: 593 17 Tien J K, Ansell G S. Resistence to Creep, Alloy and Microstructure Design, NewYork: Academic Press,1976: 167= |
|