| Al-CuAl_2共晶层片间距的数值模拟 |
| 张伟强;杨院生;胡壮麒 |
| 中国科学院金属研究所快速凝固及非平衡合金国家重点实验室;沈阳;110015;中国科学院金属研究所快速凝固及非平衡合金国家重点实验室;沈阳;110015;中国科学院金属研究所快速凝固及非平衡合金国家重点实验室;沈阳;110015 |
|
| NUMERICAL SIMULATION OF THE INTERLAMELLAR SPACING OF Al-CuAl_2 EUTECTIC |
| ZHANG Weiqiang;YANG Yuansheng; HU Zhuangqi (State Key Lab of RSA; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015) |
引用本文:
张伟强;杨院生;胡壮麒. Al-CuAl_2共晶层片间距的数值模拟[J]. 金属学报, 1998, 34(1): 1-6.
,
,
.
NUMERICAL SIMULATION OF THE INTERLAMELLAR SPACING OF Al-CuAl_2 EUTECTIC[J]. Acta Metall Sin, 1998, 34(1): 1-6.
1 Jackson A.Hunt J D,Trans Metall Soc AIME;1966; 236:1129 2 Trivedi R,Magnin P,Kurz W、Acta Metall Mater. 1987; 35: 971 3 Fisher Jt Kurz W. Acta Metall; 1980; 28: 777 4 Qunenisset M,Nalslain R, J Crystal Growth,1981;54:465 5 Magnin P,Trivedi R.Acta Metall Mater.1991:39:453 6 Jordan M,Hunt J D Metall Tarns, 1971; 2:453 7 Ourdjini A,Liu J, Elliott R.Mater,Set Technol,1994;10:312 8 Clark J N, Elliott R. Metall Trons,1976;7A:1197 9 Liu J,Elliott R.Acta Metall Mater,1995;43:3301 10 Zhang Weiqang,Liu Qingmin,Zhu Yuefeng,Yang Yuansheng,Hu Zhuangqi.Acta Metall Sin(Engl Lett),1997;10:461 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|